Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0448 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Network Polymers NPP 30-2000 TF40
Description: 40% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU (Europe-Africa-Middle East)
LNP* COLORCOMP* G1000-GY4A805-0 is a compound based on Polysulfone resin. Added features include: Custom Color Grey.
Density 1.24 g/cc
0.0448 lb/in³
(DAM); ISO 1183
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479; ASTM D792
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792B
LyondellBasell Astryn 65F4-4 Polypropylene Homopolymer, 40% Talc
Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, high stiffness, good dimensional stability, excellent heat resistanceApplications: automotive heater and..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66
LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant.
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Techmer ES Electrablend® PC 04005 FR BK Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183/A
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183-87
Wellman Wellamid® GF14-60 XE-NBK1 Nylon 6, 14% Glass Fiber Reinforced
All information provided by Wellman Engineered Resins.
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber
40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber
15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
Density 1.24 - 1.28 g/cc
0.0448 - 0.0462 lb/in³
ISO R 1183
Fainplast Compounds CKL 66 Flexible PVC, Sheathing Lead Free
General purposes
Density 1.24 g/cc
0.0448 lb/in³
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High..
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 51579XA028 0.028" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material a..
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T..
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
CENTROPLAST CENTRO HPM Polysulfone
This plastic has good hydrolysis, chemical and radiation resistance, and can operate at high temperatures. It is used in food processing industry, pumps and valves, and medical equipment.Informatio..
Density 1.24 g/cc
0.0448 lb/in³
Arkema Group Rilsan® AZM 30 O TLD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-050,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: natural. Light and heat stabilizing agent. Mold-release agent.High rigidity. High..
Density 1.24 g/cc
0.0448 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183-1-A
BASF Elastollan S 90 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Density 1.24 g/cc
0.0448 lb/in³
A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Density 1.24 - 1.28 g/cc
0.0448 - 0.0462 lb/in³
ISO R 1183
Fainplast Compounds PM 6805 Flexible PVC, Lead Free
Various profiles
Copyright © lookpolymers.com All Rights Reserved