Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Multibase Multi-Pro® 4005 M Polypropylene
Mica Filled, 40% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Nilit FRIANYL A63 TF30 Nylon 6.6 for injection molding, 30% PTFE lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Lubricomp DL002E PC (Europe-Africa-Middle East)
LNP* Lubricomp* DL002E is a compound based on Polycarbonate resin containing PTFE. Added features include: Internally Lubricated, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afric..
Density 1.25 - 1.85 g/cc
0.0452 - 0.0668 lb/in³
Average value: 1.53 g/cc Grade Count:4
Overview of materials for Phenolic, Ablative Coating
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Ablative Coating". Each property range of values reported is minimum and maximum values of app..
Density 1.25 g/cc
0.0452 lb/in³
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Mitsubishi Xantar® MX 1094 Polycarbonate-9% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Density 1.25 g/cc
0.0452 lb/in³
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC
LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp PL004 PA 6
LNP* Lubricomp* PL004 is a compound based on Nylon 6 containing PTFE Lubricant. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for the Americas region.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF20 HS BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Europe-Africa-Middle East)
LNP* STATLOY* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant. Added features include: Permanent Antistatic, Flame Retardant.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Tipco Tipcolene® FPM 40 - 40% Mica Reinforced Polypropylene Homopolymer, High Stiffness
40% Mica Reinforced PP HomopolymerApplications: Electrical & AutomotiveProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Density 1.25 g/cc
0.0452 lb/in³
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D 792
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D 792
Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled
PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Density 1.25 g/cc
0.0452 lb/in³
Covestro Bayblend® T 88-4N Polycarbonate/ABS Blend, 20% Glass Fiber
Contains 20% glass fiber reinforcement, high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – ..
Density 1.25 g/cc
<br>@Thickness >=0.000 mm
0.0452 lb/in³
<br>@Thickness >=0.000 in
24hr/23°C/50% RH; ISO 1183-A; IEC/EN 61212-2 7.3
Elektro-Isola Etronit B 66 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: Specially designed for high-voltage insulation with high requirements for insulating capacity along the tube.Applications: Insulating tubes in high-voltage switchgear and tap changers....
Density 1.25 g/cc
0.0452 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66 &nbsp;(Unverified Data**)
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p..
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds GS 7512 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.25 g/cc
0.0452 lb/in³
Calculated from nominal thickness and yield
DuPont Teijin Films Mylar® RL43 Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® RL43 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer. Mylar® RL43 is designed to produce stro..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Makrofol BL 2-4 820816 is a translucent dazzle free extruded film based on Makrolon, the High Tech Polycarbonate of Bayer MaterialScience. It comprises excellent punching performance combined with h..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0339W40L Wollastonite Reinforced
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Conditioned, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Density 1.25 g/cc
0.0452 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic..
Density 1.25 g/cc
0.0452 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value..
Density 1.25 g/cc
0.0452 lb/in³
Loctite® 572 Low Strength Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
Density 1.25 g/cc
0.0452 lb/in³
Loctite® 549 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
Density 1.25 g/cc
0.0452 lb/in³
DuPont Performance Polymers Neoprene TRT Polychloroprene Rubber &nbsp;(discontinued **)
Neoprene Type TRT is a polychloroprene/2,3 dichloro 1,3-butadiene copolymer, has excellent polymer stability, and a very slow crystallization rate. Physical form: Chips. Color: Silver Gray to ligh..