Polymer Property : Density = 0.0459 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Density 1.27 g/cc
0.0459 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Density 1.27 - 1.75 g/cc
0.0459 - 0.0632 lb/in³
Average value: 1.57 g/cc Grade Count:131
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Eastman Eastar GN002 Copolyester, Natural  (discontinued **)
Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha..
Density 1.27 g/cc
0.0459 lb/in³
Eastman Eastar GN101 PETG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Density 1.27 g/cc
0.0459 lb/in³
Eastman Tenite 131E-28 Cellulose Acetate  (discontinued **)
28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
FKuR Kunststoff Bio-Flex® F 2110 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors.
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66
LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem 1010RV PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Techmer ES Elastoblend® PA6 GF25 IM HS L BK 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE
High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method).
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Techmer ES HiFill FR® PA6/6 FR 344
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc.
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Techmer ES Luriblend® PA4/6 HS TL15
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc...
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA 11 (Asia Pacific)
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing Glass Bead.
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DX03633C PC
LNP STAT-KON* DX03633C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate
Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.27 - 1.31 g/cc
0.0459 - 0.0473 lb/in³
ISO R 1183
Fainplast Compounds CKL 0252/R Flexible PVC, Sheathing Lead Free
Mineral oil resistant sheathing
Density 1.27 g/cc
0.0459 lb/in³
ISO R1183
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Aclo Accutech Nylon 6 NY0730G20L Glass Reinforced
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..