Polymer Property : Density = 0.0473 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics EXTEM XH1005 TPI Resin
Thermoplastic Polyimide Extem* XH1005 Resin.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Polykemi AB POLYshine PBT D211 PBT, Modified
Information provided by Polykemi AB
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® S600F20 NC010 PBT  (Unverified Data**)
Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 (Asia Pacific)
LNP* Stat-loy* 9X03508 is a compound based on PPO+PA66 resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant, High Impact.
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 PPS
LNP* THERMOCOMP* 9X04488 is a compound based on PPS resin containing Mineral.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC
LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable.
Density 1.31 g/cc
0.0473 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp ZF-1006 BK8-950 PPE+PS
LNP* Thermocomp* ZF-1006 BK8-950 is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermotuf PK005EI2 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* PK005EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Polyplastics Duranex® 800FP Polybutylene Terephthalate (PBT), Unfilled PBT for film, Extrusion, Super High Viscosity
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Tipco Tipcolene® FPT 20 FR VO PPC - UL94-V0 Flame Retardant, 20% Talc Polypropylene Copolymer
20% Talc Reinforced PP CopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Density 1.31 g/cc
0.0473 lb/in³
ASTM-D792
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled
Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Polyplastics Duranex® CA7200NX Polybutylene Terephthalate (PBT), Antistatic
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30
Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In..
Density 1.31 g/cc
0.0473 lb/in³
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by ..
Density 1.31 g/cc
0.0473 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® RS 30G30HSL BK038A Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Information provided by DuPont Performance Polymers
Density 1.31 g/cc
0.0473 lb/in³
A. Schulman ComAlloy Hiloy® 243 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.31 g/cc
0.0473 lb/in³
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona..