| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 - 1.34 g/cc | 0.0347 - 0.0484 lb/in³ | Average value: 1.07 g/cc Grade Count:42 |
|
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
|
|||
| Density | 1.21 - 1.34 g/cc | 0.0437 - 0.0484 lb/in³ | Average value: 1.29 g/cc Grade Count:8 |
|
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | Fusor 2201 |
|
Lord Adhesives Fusor® 2200 / 2201 Urethane Adhesive
Fusor® 2200/2201 is a black equal-mix, twocomponent, paste urethane adhesive system. Fusor 2200/2201 adhesive bonds FRP, SMC, and other plastics with little surface preparation where bond strengt..
|
|||
| Density | 1.18 - 1.34 g/cc | 0.0426 - 0.0484 lb/in³ | |
|
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of ..
|
|||
| Density | 1.28 - 1.34 g/cc | 0.0462 - 0.0484 lb/in³ | |
|
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FK 76 Flexible PVC, Insulation Lead Free
General purposes
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 7816 Flexible PVC, Injection Molding for Footwear
Soles for mild climates
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CL 65 Flexible PVC, Sheathing
General purposes
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding
Anti-impact connectors and components
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 5540 Flexible PVC, Extrusion
Gaskets for frames
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 9012 Flexible PVC, Extrusion
Furniture border
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1184 |
|
Fainplast Compounds KL 96/1 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 6045 Flexible PVC, Lead Free
Gaskets for frames
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FKA 97 Flexible PVC, Flame Retardant Insulation Lead Free
Telephonic insulation
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 8020 Flexible PVC, Lead Free
Covering steel sheaths
|
|||
| Density | 1.30 - 1.34 g/cc | 0.0470 - 0.0484 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 8030 Flexible PVC, Lead Free
Furniture border
|
|||