Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0491 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Polykemi AB SCANAMID 66 A11^ X30 LS Nylon 66, Glass Reinforced, Laser Printable
Information provided by Polykemi AB
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.36 g/cc
0.0491 lb/in³
DIN 53479; ASTM D792
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
LATI LAPEX A Polyethersulfone (PES) (UL94 V-0)  (Unverified Data**)
Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Lanxess Durethan® BG 30 X H2.0 901510 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers/glass spheres, good surface, good heat-ageing resistance
Density 1.36 g/cc
0.0491 lb/in³
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
Density 1.36 g/cc
0.0491 lb/in³
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183/A
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY
TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit..
Density 1.36 - 1.40 g/cc
0.0491 - 0.0506 lb/in³
Fiber Density
SGL Carbon Group PANOX® FM C063 EEA Oxidized Textile Fiber, Crimped staple fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.36 - 1.40 g/cc
0.0491 - 0.0506 lb/in³
Fiber Density
SGL Carbon Group PANOX® FM C063 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%) and Silicone LubricantFeatures: LubricatedAppearance: Natural ColorPro..
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Techmer ES Luriblend® PA6 GF15 TL15 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilized and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp RFC16 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RFC16 is a compound based on PA 66 resin containing Glass Fiber, Carbon Fiber. Added features include: Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Polyplastics Duranex® 2002 Polybutylene Terephthalate (PBT), Low friction, Low wear
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Washington Penn Medium Impact Copolymer 50% Talc Filled
Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi..
Density 1.36 g/cc
0.0491 lb/in³
Zircar Refractory Composites RSLE-56 MOLDABLE Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-56 Moldable is a high silica fiber reinforced ceramic composite material that is easily cut and formed into flat sheets in addition to a wide variety of simple and ..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792, ISO 1183
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
Characteristics: 30% glass fibre filled
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar.
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Eurotec® Tecomid® NB40 GB30 NL PA6, 30% glass bead reinforced, natural
Information provided by Eurotec®
Density 1.36 g/cc

@Temperature 23.0 °C
0.0491 lb/in³

@Temperature 73.4 °F
ISO 1183
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry)
Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability.
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Ashley Polymers Ashlene® 830LS-30G Nylon 6, 30% Glass Reinforced
A 30% glass fiber reinforced Nylon 6 with heat stabilizer designed to provide a high flexural modulus and good dimensional stability while maintaining the ease of processing associated with Nylon 6 ..
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
Density 1.36 g/cc
0.0491 lb/in³
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792A
Resinoid 2018 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Copyright © lookpolymers.com All Rights Reserved