Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0499 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792, ISO 1183
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66
Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylon® N1033HL Nylon 6/6 (DAM)
Information provided by Ravago.
Density 1.38 g/cc
0.0499 lb/in³
±0.02 g/cm³; DIN 53479
PolyOne Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66)
Information provided by PolyOne
Density 1.38 g/cc
0.0499 lb/in³
(DAM); ISO 1183
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin
Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume ..
Density 1.38 g/cc
0.0499 lb/in³
LATI Latilub 66-01M G/30 PA66, 30% Glass Fiber Reinforced, Molybdenum disulphide Filled
Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183/A
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183/A
Solvay TECHNYL® C 216 V35 Black Z PA6, 35% glass fiber, Conditioned
Description: Polyamide PA6 , reinforced with 35 % of glass fiber, for injection molding.Available in: North AmericaProduct Applications: It has good mechanical properties, it is used in all sectors ..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT
LNP* LUBRICOMP WL002 is a compound based on PBT resin containing 10% PTFE. Added feature of this grade is: Wear Resistant.
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber
KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated TPCI# 8263101Information provided by TP Composit..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF33 LE BK 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesAppearance: BlackTPCI#7762101Information provided by TP Compos..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Techmer ES Luriblend® PA6 CF30 TL15 BK 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: Low Friction, Good Wear Resistance and LubricatedAppearance: ..
Density 1.38 g/cc
0.0499 lb/in³
DIN 53479
Polyram PlusTek PA303G33 Nylon 6.6, 33% Glass Fiber
33% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.38 g/cc
0.0499 lb/in³
ASTM-D792
Polyram Polytron A30N02 Nylon 66, 30% Long Fiber
30% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled
injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
DSM Akulon® K224-G6U (Dry) 33% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene
Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed..
Density 1.38 g/cc
0.0499 lb/in³
DIN 53 479
Ensinger TECASINT 3022 Polyimide, Black, 15% Graphite (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i..
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded
PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
Density 1.38 g/cc
0.0499 lb/in³
(Dry)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Density 1.38 - 1.81 g/cc
0.0499 - 0.0654 lb/in³
Average value: 1.50 g/cc Grade Count:53
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Copyright © lookpolymers.com All Rights Reserved