| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Average value: 1.35 g/cc Grade Count:8 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Density | 1.06 - 1.38 g/cc | 0.0383 - 0.0499 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
|
|||
| Density | 1.15 - 1.38 g/cc | 0.0415 - 0.0499 lb/in³ | Average value: 1.20 g/cc Grade Count:8 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
|
|||
| Density | 1.30 - 1.38 g/cc | 0.0470 - 0.0499 lb/in³ | Average value: 1.34 g/cc Grade Count:3 |
|
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RKT 226 Rigid PVC, Extrusion Lead Free
Metal effect profiles
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free
Transparent profiles
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free
Electric antishock fittings
|
|||
| Density | 1.36 - 1.38 g/cc | 0.0491 - 0.0499 lb/in³ | Fiber Density |
|
SGL Carbon Group PANOX® FB M400 EEA Oxidized Textile Fiber, Milled Fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
|
|||
| Density | 1.36 - 1.38 g/cc | 0.0491 - 0.0499 lb/in³ | Fiber Density |
|
SGL Carbon Group PANOX® FB T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CKL 8318/2 Flexible PVC, Sheathing Lead Free
Sheathing coaxial TV cables
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 89/2 Flexible PVC, Insulation
Insulation for special application
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 100/2 Flexible PVC, Injection Molding, Lead Free
Semi-rigid for cable passage
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO 1183 |
|
Fainplast Compounds Hax™ HFX 519 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com..
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds HLA 075 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds ARC 10 Rigid PVC, Atoxic for General Purpose
Bottles medium antishock
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds ARC 20 Rigid PVC, Atoxic for General Purpose
Bottles medium/high antishock
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose
Bottles very high antishock
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GA 75/R Flexible PVC, Flame Retardant Sheathing
According to UL 1581 Class 43 (90°C)
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds HL 91 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds KL 101 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 80°C
|
|||
| Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
|
|||
| Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow..
|
|||
| Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium..
|
|||
| Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec..
|
|||
| Density | 1.32 - 1.38 g/cc | 0.0477 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
|
|||
| Density | 1.35 - 1.38 g/cc | 0.0488 - 0.0499 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric ..
|
|||
| Density | 1.28 - 1.38 g/cc | 0.0462 - 0.0499 lb/in³ | Average value: 1.32 g/cc Grade Count:7 |
|
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds KL 96 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 105°C
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free
Transparent antishock profiles
|
|||
| Density | 1.34 - 1.38 g/cc | 0.0484 - 0.0499 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CL 76/1 Flexible PVC, Sheathing
General purposes
|
|||