| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.44 - 1.91 g/cc | 0.0520 - 0.0690 lb/in³ | |
|
Parker Chomerics CHO-SHIELD® 4076-50A Conductive Coating
Conductive Nickel-Filled Coating. This is an electrically conductive waterborne nickel-filled polyurethane coating that provides excellent shielding against radiated EMI. It bonds well to plaster, c..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO data |
|
BASF Capron® GR40 HS 40% Glass-Filled Nylon 6 (Dry)
(discontinued **)
Capron GR40 HS is a heat stabilized 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stabil..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792, ISO 1183 |
|
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | Crystalline; ISO 1183 |
|
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
|
|||
| Density | 1.44 - 1.48 g/cc | 0.0520 - 0.0535 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RH 212/W Rigid PVC, Antishock Extrusion
Outdoor antishock profiles
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | |
|
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP IFP36 PA6.12
LNP* LUBRICOMP* IFP36 is a Nylon 6/12 base resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of t his grade include: Wear Resistant.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP RL0039XP PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RL0039XP is a compound based on PA66 resin containing PTFE, Flame Retardant. Added features include ; Flame Retardant, internally Lubricated.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® POM CO GF5 CC 5% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 5% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP UX05504 PPA (Asia Pacific)
LNP* THERMOCOMP* UX05504 is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP VERTON RX03013 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX03013 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183-87 |
|
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66
Description: Post Consumer Compound Nylon 66Information provided by Wellman.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | |
|
Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced
Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | dry; ISO 1183 |
|
DSM Akulon® SG-KGS6 PA66-GF30 FR
30% Glass Reinforced, Halogen free and free of red phosphorous
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40
Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | Cured |
|
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
Eurostar Star L PA66 30V D61 PA66, Glass Fiber Filled, Injection Molded
Star L PA66 30V D31 is a PTFE/Silicone Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
Eurostar Starflam RFB247EX PA66/6, Glass Bead/Fiber Filled, Flame Retardant, Injection Molded
RFB247EX is a Halogen Free and Red Phosphorous Free Flame Retardant, Glass Bead/ Glass Fiber Reinforced Polyamide 66/ Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.44 - 1.48 g/cc | 0.0520 - 0.0535 lb/in³ | ISO R 1184 |
|
Fainplast Compounds HGK 82 Flexible PVC, Sheathing for High Temperatures Lead Free
Operating temperature 90°C
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
Barlog Plastics KEBAFORM C 903 LF POM Copolymer unreinforced, improved wear and friction
POMInformation provided by BARLOG plastics GmbH.
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
|
E-Polymers Tekaloy® G70GFR , Flame Retardant, 30% Glass Fiber Reinforced PC/ABS Alloy
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
|
|||
| Density | 1.44 - 1.54 g/cc | 0.0520 - 0.0556 lb/in³ | Average value: 1.51 g/cc Grade Count:39 |
|
Overview of materials for Polycarbonate, 40% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | |
|
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film
All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
|
Plenco 7697 Phenolic, Granular, Compression Molded
PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ISO 1183 |
|
Polyplastics Duracon® CH-10 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Density | 1.44 g/cc | 0.0520 lb/in³ | ASTM D792 |
|
Techmer ES HiFill FR® PA6/6 GF15 FR BK 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear..
|
|||