| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Kadel® E-1230 Polyketone
(discontinued **)
Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, p..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
LATI LAESTRA G/30-V0CT1 30% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS)
Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | (DAM); ISO 1183 |
|
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Cond)
(discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Density |
1.45
g/cc <br>@Temperature 23.0 °C
|
0.0524
lb/in³ <br>@Temperature 73.4 °F
|
ISO 1183 |
|
Inno-Comp INNOBATCH® PPH 3260 60% Chalk-Filled Polypropylene Homopolymer
INNOBATCH® PPH 3260 is a 60% chalk-filled polypropylene homopolymer based masterbatch. This grade is available in nature form.These products that are offered under the brand name INNOBATCH® ar..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | Dry; ISO 1183 |
|
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | Dry; ISO 1183 |
|
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Solvay Specialty Polymers Amodel® DW-1130 Polyphthalamide (PPA), 30% Glass Fiber
Amodel® DW-1130 is a 30% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient o..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East)
VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles.
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP KX97390 Acetal Copolymer
LNP THERMOCOMP* KX97390 is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Chemically Coupled.
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA
LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
DSM Arnite® TV6 240 PBT-GF20
20% Glass Reinforced
|
|||
| Density | 1.45 - 1.51 g/cc | 0.0524 - 0.0546 lb/in³ | |
|
Dow BETAMATE™ 5103-2 Epoxy
BETAMATE™ 5103-2 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel, including coated ste..
|
|||
| Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 80 Flexible PVC, Insulation
General purposes
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR430A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO 1183 |
|
Fainplast Compounds Hax™ HFX 500 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Standard sheathingInformation provided by Fainplast Compou..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183/A |
|
Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled
Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast.
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.45 - 1.49 g/cc | 0.0524 - 0.0538 lb/in³ | ISO 1183 |
|
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 Method A |
|
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
|
Polyplastics Duracon® CH-15 Acetal Co-polymer (POM), Conductive, CF reinforced, Wear resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Density | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
|
Plenco 7467 Phenolic, Nodular, Transfer Molded
(discontinued **)
Two-Stage Phenolic. PLENCO 07467 is an organic phenolic molding compound offering excellent dimensional stability under conditions of total water immersion. 07467 is formulated to provide improved ..
|
|||