| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.51 g/cc | 0.0546 lb/in³ | STN 64 0111 |
|
Plastcom SLOVASTER® B GF 20 FRK 3 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | DIN 53479 |
|
Qualchem Danamid FGF-50 Polyamide 6, 50% Glass Fiber
Reinforced with glass fiber.Information provided by Qualchem Zrt.
|
|||
| Density | 1.51 - 1.70 g/cc | 0.0546 - 0.0614 lb/in³ | Average value: 1.60 g/cc Grade Count:5 |
|
Overview of materials for PCT, 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
PolyOne Edgetek® AM-35GF/000 FR NH Polyphthalamide (PPA)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
|
Manifattura Cattaneo VESPEL® SP21 Polyimide
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183/A |
|
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66
LNP* LUBRICOMP* RFL36XXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFN18SXS PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFN18SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Asia Pacific)
LNP* THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES (Asia Pacific)
LNP* Thermocomp* JF004EXP is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA 6/10 (Europe-Africa-Middle East)
LNP* Thermocomp* QF00A is a compound based on Nylon 6/10 resin containing Glass Fiber.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
Tisan TISESTER® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183-87 |
|
Wellman Wellamid® GF43-66 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | Nominal Laminate |
|
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K
Fiber: AS7, Weave: UD, 134 g/m2Information provided by HexCel
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Density |
1.51
g/cc @Temperature 23.0 °C |
0.0546
lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
|
Ensinger TECASINT 1611 Polyimide, 30% PTFE Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | |
|
Arkema Group Lucalor® PEY 333 CPVC, Pipe Grade
LUCALOR PEY 333 is a chlorinated polyvinyl chloride compound (CPVC) developed for the extrusion of pipes for hot water supply and distribution system.ISO data provided by the manufacturer, Arkema.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Conditioned, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | |
|
DuPont Performance Polymers Sorona® 2045G BK346A Polytrimethylene Terephthalate (PTT)
(Unverified Data**)
45% Glass Reinforced Polytrimethylene TerephthalateInformation provided by DuPont Performance Polymers
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**)
45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
|
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Density | 1.51 g/cc | 0.0546 lb/in³ | Crystaline; ISO 1183 |
|
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..
|
|||