Polymer Property : Density = 0.0549 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792, ISO 1183
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East)
Extem XH2315 Resin
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Density 1.52 g/cc
0.0549 lb/in³
Momentive Performance Materials IGS3713-D1 Insulating Glass Sealant, Black
One-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Cure Method: Alkoxy (Neutral). Tack-free time 0.5 hr. Peel Strength 50 lb/in. ..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer
LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear
LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI
LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP JF004ER PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF-1004 S-3 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA
LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific)
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Density 1.52 g/cc
0.0549 lb/in³
As Cast
Zircar Ceramics ZIRALCAST 95 Alumina Refractory Castable
Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applica..
Density 1.52 g/cc
0.0549 lb/in³
Laminate
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel
Density 1.52 g/cc
0.0549 lb/in³
Loctite® 3563 Epoxy Snap Cure Underfill
COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Polyplastics Duranex® 7307B Polybutylene Terephthalate (PBT), Super low warpage, GB filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Density 1.52 - 1.56 g/cc
0.0549 - 0.0564 lb/in³
ISO R 1183
Fainplast Compounds GK 87 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
Density 1.52 - 1.55 g/cc
0.0549 - 0.0560 lb/in³
MIL-PRF-81733D
3M AC-665 Class C-48 Aerospace Sealant
3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)
Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry)
Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Applied Composites 150 Polyester SMC
Industry Application: TransportationProduct Application: Engine CoversDistinct Features: Grey Pigments Only, Low DensityInformation provided by Applied Composites Corporation.
Density 1.52 g/cc
0.0549 lb/in³
A. Schulman ComAlloy Hiloy® 432 Glass Reinforced, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..
Density 1.52 - 1.56 g/cc
0.0549 - 0.0564 lb/in³
ISO R 1184
Fainplast Compounds RE 220 Rigid PVC, Extrusion
Various profiles
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Plaslok 306 Black General Purpose Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 306 is a two-stage, mineral and flock..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10
LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti..