Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0607 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183-1
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)
Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
SABIC Innovative Plastics LNP FARADEX KX98009 Acetal Copolymer (Europe-Africa-Middle East)
LNP* FARADEX* KX98009 is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber, Glass Fiber. Added features include : EMI / RFI Shielding, Electrically Conductive.
Density 1.68 g/cc
0.0607 lb/in³
ASTM D3275
Solvay Specialty Polymers Halar® 3404DA Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Halar® 3404DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug and Cosmetic Act food additive regulation ..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D3275
Solvay Specialty Polymers Halar® 6014F Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)&
Halar® 6014F is a clear, semi-crystalline melt processable fluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in protection and..
Density 1.68 g/cc
0.0607 lb/in³
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Density 1.68 g/cc
0.0607 lb/in³
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Density 1.68 g/cc
0.0607 lb/in³
IDI Composites E-207 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183/A
Solvay TECHNYLSTARâ„¢ SX 216 L2 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, UV stabilized and characterized by a high fluidity of the melt, for injection molding.Available in: Europe and North America Pr..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Solvay Specialty Polymers Ajedium™ Films -- Halar® 500LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Halar® ECTFE is a semi-crystalline fluoropolymer with a chemical structure of a 1:1 alternating copolymer of ethylene and chlorotrifluoroethylene.Halar® film is a strong, hard, tough, abrasion..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Solvay Specialty Polymers Halar® 1450LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Polyme..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D1505
Solvay Specialty Polymers Halar® 3404DA Ethylene Chlorotrifluoroethylene Copolymer (ECTFE), Filled
Halar® 3404DA is a filled, pearl-white, semicrystalline melt processable fluorinated resin that may be used in full compliance with the federal Food, Drug and Cosmetic Act food additive regulatio..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber
Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Solvay Specialty Polymers Ryton® R-4-280BL Polyphenylene Sulfide (PPS), Glass Fiber
Ryton® R-4-280BL 40% glass fiber reinforced polyphenylene sulfide compound provides a combination of enhanced mechanical strength and good flow for injection molding.Features: Good Chemical Resis..
Density 1.68 g/cc
<br>@Temperature 25.0 °C
0.0607 lb/in³
<br>@Temperature 77.0 °F
Solvay Specialty Polymers Galden® SV80 PFPE Solvent
Galden® SV grades are specifically recommended for use as solvents.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF55 HS L 55% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF55 HS L BK 55% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific)
LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - LINEAR
LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing 40% Glass Fiber. Added features of this material include: Easy Molding.
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Techmer ES HiFill® PPA GF33 FR HS L 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Vyncolit X7255 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. Very easy to transform in complex shapes. Excellent mechanical and thermal properties. Higher isotropic properties and good dimensional s..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Westlake Plastics ECTFE Film Made from HALAR® Ethylene-chlorotrifluoroethylene Resin
Excellent purity. Excellent chemical resistance. Low permeability. Excellent abrasion resistance. Excellent temperature resistance.Halar® is a trade name of Solvay Solexis, Inc. Information p..
Density 1.68 - 1.72 g/cc
0.0607 - 0.0621 lb/in³
IEC 60811
Fainplast Compounds HAX HF 108 Halogen Free PVC
Filling and bedding, designed to meet BS 6724
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
BASF Petra® 130 FR 30% Glass Filled PET
Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail..
Density 1.68 g/cc
0.0607 lb/in³
BASF Heligoen® Blue L 6700 F Color Additive
Chemical Structure: Cu-phthalocyanine, Epsilon Application: Pigment for PaintsPhysical form: PowderInformation provided by BASF
Density 1.68 g/cc
0.0607 lb/in³
ASTM D3275
Solvay Specialty Polymers Halar® 6514 Polyethylene, Chlorotrifluoroethylene (ECTFE) &nbsp;(Unverified Data**)&l
Halar 6514 is a black, semi-crystalline melt processable fluorinated primer. It is designed to be applied directly to substrates by electrostatic or fluidized bed techniques. In particular Halar 651..
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Vyncolit W5020 Glass Filled Novolac Phenolic
Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform..
Density 1.68 g/cc
0.0607 lb/in³
ASTM D792
Techmer ES HiFill® PA4/6 GF30 FR HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Flame Retardant and Lu..
Copyright © lookpolymers.com All Rights Reserved