| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.70 - 1.75 g/cc | 0.0614 - 0.0632 lb/in³ | |
|
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds
Isoflow Graphite Rings facilitate an even flow of oil around the circumference of the billet. This even flow results in improved billet surface quality over long casting campaigns. Isoflow Graphit..
|
|||
| Density | 1.13 - 1.75 g/cc | 0.0408 - 0.0632 lb/in³ | Average value: 1.48 g/cc Grade Count:151 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
|
|||
| Density | 1.27 - 1.75 g/cc | 0.0459 - 0.0632 lb/in³ | Average value: 1.57 g/cc Grade Count:131 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
|
|||
| Density | 1.35 - 1.75 g/cc | 0.0488 - 0.0632 lb/in³ | Average value: 1.60 g/cc Grade Count:76 |
|
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
|
|||
| Density | 1.65 - 1.75 g/cc | 0.0596 - 0.0632 lb/in³ | ASTM D792 |
|
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **)
Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
|
|||
| Density | 1.28 - 1.75 g/cc | 0.0462 - 0.0632 lb/in³ | Average value: 1.43 g/cc Grade Count:232 |
|
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
|
|||
| Density | 1.14 - 1.75 g/cc | 0.0412 - 0.0632 lb/in³ | Average value: 1.45 g/cc Grade Count:186 |
|
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Density | 0.890 - 1.75 g/cc | 0.0322 - 0.0632 lb/in³ | Average value: 1.37 g/cc Grade Count:108 |
|
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
|
|||
| Density | 1.45 - 1.75 g/cc | 0.0524 - 0.0632 lb/in³ | |
|
Solvay Polishing Opalineâ„¢
Description: Polishing OPALINE® is a high quality cerium oxide powder developed high precision polishing. It has an excellent surface quality, very low roughness, and has quality consistency. The..
|
|||
| Density | 1.60 - 1.75 g/cc | 0.0578 - 0.0632 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
|
|||
| Density | 1.63 - 1.75 g/cc | 0.0589 - 0.0632 lb/in³ | Molding; IS 867-1963 |
|
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown..
|
|||
| Density | 1.55 - 1.75 g/cc | 0.0560 - 0.0632 lb/in³ | Molded |
|
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf..
|
|||
| Density | 1.70 - 1.75 g/cc | 0.0614 - 0.0632 lb/in³ | |
|
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Density | 1.41 - 1.75 g/cc | 0.0509 - 0.0632 lb/in³ | Average value: 1.54 g/cc Grade Count:3 |
|
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
|
|||
| Density | 1.32 - 1.75 g/cc | 0.0477 - 0.0632 lb/in³ | Average value: 1.59 g/cc Grade Count:68 |
|
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
|
|||
| Density | 1.34 - 1.75 g/cc | 0.0484 - 0.0632 lb/in³ | Average value: 1.51 g/cc Grade Count:91 |
|
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..
|
|||
| Density | 1.30 - 1.75 g/cc | 0.0470 - 0.0632 lb/in³ | Average value: 1.43 g/cc Grade Count:40 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..
|
|||