Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0639 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a..
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy
The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1100 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 g/cc
0.0639 lb/in³
SGL Carbon Group EK 2209 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill FR® TPX-PBT-00014 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Density 1.77 g/cc

@Temperature 25.0 °C
0.0639 lb/in³

@Temperature 77.0 °F
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 0177 Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill® PVDF CF15 BK 15% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 15% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF60 TL10 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 8575101Information provi..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade
Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resista..
Density 1.77 g/cc
0.0639 lb/in³
UCAR Carbon UCAR® CSX Extruded Graphite
Densified prior to graphitization, Grade CSX is an extruded graphite, higher in strength and lower in permeability than CS. It is a material for applications requiring higher densities, better mecha..
Density 1.77 g/cc
0.0639 lb/in³
Relative Density; ISO 1183
Vyncolit 2923 W Novolac Phenolic
Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Plenco 6500 Phenolic, Briquette, Injection Molded
PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 ..
Density 1.77 g/cc
0.0639 lb/in³
(DAM); ISO 1183
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
Information provided by DSM Engineering Plastics.
Density 1.77 g/cc
0.0639 lb/in³
(DAM); ISO 1183
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Density 1.77 g/cc
0.0639 lb/in³
Cytec Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Density 1.77 g/cc
0.0639 lb/in³
Arkema Group Kynar® 1000 HDC N 118 PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig..
Density 1.77 g/cc
0.0639 lb/in³
Nominal Laminate
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581
Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel
Density 1.77 g/cc
0.0639 lb/in³
ASTM D-792
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac
FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat..
Copyright © lookpolymers.com All Rights Reserved