Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0647 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1100 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1700 High Viscosity PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 850 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1000 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1300 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 2950 PVDF Copolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..
Density 1.75 - 1.79 g/cc
0.0632 - 0.0647 lb/in³
ISO R 1183
Fainplast Compounds CR 85 Flexible PVC, Electrical Bedding
Bedding
Density 1.59 - 1.79 g/cc
0.0574 - 0.0647 lb/in³
Molded
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing ..
Density 1.59 - 1.79 g/cc
0.0574 - 0.0647 lb/in³
Molded
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound
BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Density 1.41 - 1.79 g/cc
0.0509 - 0.0647 lb/in³
Average value: 1.61 g/cc Grade Count:10
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Density 1.48 - 1.79 g/cc
0.0535 - 0.0647 lb/in³
Average value: 1.64 g/cc Grade Count:22
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..