Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0665 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.64 - 1.84 g/cc
0.0592 - 0.0665 lb/in³
Average value: 1.71 g/cc Grade Count:30
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Density 1.80 - 1.84 g/cc
0.0650 - 0.0665 lb/in³
ISO R 1183
Fainplast Compounds CRK 84 Flexible PVC, Electrical Bedding Lead Free
Bedding
Density 1.80 - 1.84 g/cc
0.0650 - 0.0665 lb/in³
ISO R 1183
Fainplast Compounds CRKA 87 Flexible PVC, Flame Retardant Electrical Bedding Lead Free
Flame retardant bedding
Density 1.82 - 1.84 g/cc
0.0658 - 0.0665 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 75-1 Polypropylene Homopolymer, 75% Calcium Carbonate
Information provided by PolyPlastic Group.
Density 0.886 - 1.84 g/cc
0.0320 - 0.0665 lb/in³
Average value: 0.918 g/cc Grade Count:172
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Density 1.24 - 1.84 g/cc
0.0448 - 0.0665 lb/in³
Average value: 1.45 g/cc Grade Count:8
Overview of materials for Polypropylene w/ 50% Calcium Carbonate
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and ..
Copyright © lookpolymers.com All Rights Reserved