| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Green Density |
|
Nabaltec NABALOX® NO 615-30 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Green Density |
|
Nabaltec NABALOX® NO 625-31 Reactive Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
|
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate
Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Indium Corp. Indalloy 192 Pure Aluminum
Information Provided by Indium Corporation
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent |
|
Gouda Vuurvast AK 80 FM Dense Refractory Brick
Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Apparent |
|
Gouda Vuurvast AK 82 A Dense Refractory Brick
Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Schott S8802 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP WH0270B PBT (Asia Pacific)
LNP THERMOCOMP* WH0270B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Toho Tenax Besfight® MC Type I (3000 Filament) Nickel Coated Carbon Fiber
Besfight MC Polyacrylonitrile (PAN) based fiber combines the mechanical properties and flexibility of carbon fiber with the electrical conductivity of nickel. It does not delaminate even at the mec..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Goodfellow Aluminum 99/Silicon 1 Alloy
An addition of 1% Silicon lowers the melting range without producing brittleness. Aluminum/Silicon alloys are used in brazing alloys and welding wire for joining Aluminum as well as bonding wire in ..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
American Elements Aluminum Nanoparticles
General DescriptionAluminum (Al) Nanoparticles, nanodots or Nanopowder are black spherical high surface area metal particles. Nanoscale Aluminum Particles are typically 10-30 nanometers (nm) with sp..
|
|||
| Density | 2.70 - 2.90 g/cc | 0.0975 - 0.105 lb/in³ | |
|
Tritex TREO Needled Blanket Insulation
Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Cured |
|
Chesterton ARC MX1 Vertical Build Extreme Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”)..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | Cured |
|
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-10 Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-12 Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
Anderman Ceramics EC100P Recrystallized Silicon Carbide
EC100P is a porous silicon carbide with excellent thermal shock resistance and high strength and high temperature operating capabilities up to 2910 °F (1600 °C). It is excellent for use in furnace..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-11 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-12 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-30 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-62 Industrial Woven Fabric 312
Information provided by 3M
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ 312 Industrial Ceramic Fiber
Chemical composition above is wt%. Crystal phase is mullite + amorphous (or 100% amorphous). Filament diameter is 10-12 µm.3M Nextel fibers 312, 440, and 550 are designed for non-structural appli..
|
|||
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
|
3M Nextel™ AF-14 Industrial Woven Fabric 312
Information provided by 3M
|
|||