| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.60 - 3.65 g/cc | 0.130 - 0.132 lb/in³ | Sintered Density |
|
Nabaltec GRANALOX® NM 9216 Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | Sintered Density |
|
Nabaltec NABALOX® NO 115-71 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Nabaltec NABALOX® NO 201 Calcined Aluminum Oxide
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Nabaltec NABALOX® NO 201P Soft Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | Sintered Density |
|
Nabaltec NABALOX® NO 315 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
NanoScale NanoActive® Magnesium Oxide Plus
NanoActive MgO is produced using proprietary processes to obtain very high specific surface area (over 600 m2/g), small crystallite size, high porosity material possessing high chemical reactivity a..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | calculated from bulk density after subtracting pore volume |
|
MarkeTech Repton 115 Aluminum Oxide
Brand 115 features: High Density and Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even whe..
|
|||
| Density | 3.61 g/cc | 0.130 lb/in³ | calculated from bulk density after subtracting pore volume |
|
MarkeTech Repton 314 Mullite
Brand 314 features: Superior hot creep.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when the..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
MarkeTech Spinel (MgAl2O4) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 9%.
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Schott F2 Glass
Information Provided by SCHOTT North America, Inc.
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Schott F2HT Glass
Information Provided by SCHOTT North America, Inc.
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
CeramTec 771 94% Alumina (Al2O3)
Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America.
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
American Elements Magnesium Oxide Nanopowder
General DescriptionMagnesium Oxide Nanoparticles or Magnesia Nanoparticles (MgO) Nanoparticles, nanodots or nanopowder are spinel, high surface area particles. Nanoscale Magnesium Oxide Nanoparticle..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | ASTM C20 |
|
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | ASTM D1475 |
|
Aptek 2312-PMF Electrically conductive, low modulus adhesive
Premixed-frozen, electrically conductive, low modulus adhesiveAPTEK 2312-PMF is a one component, premixed-frozen, silver filled, electrically conductive soft paste adhesive. It is designed to bond m..
|
|||
| Density | >= 3.60 g/cc | >= 0.130 lb/in³ | |
|
Advanced Ceramics ALC 1081 (C-786) Alumina
Information provided by Advanced Ceramics Limited (ACL)
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
BASF Paliotan® Yellow L 2045 Color Additive
Description: Pigment combination based on Bismuth VanadatSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Amine curing system and Airdrying systems.Information provided b..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Loctite® 3883 Stencil Print Isotropic Epoxy Adhesive
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona..
|
|||
| Density | 3.60 g/cc | 0.130 lb/in³ | |
|
Loctite® 3889 Rapid Cure Isotropic Epoxy Adhesive
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona..
|
|||
| Density | 3.61 g/cc | 0.130 lb/in³ | |
|
Schott GG395 Long Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG385, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630..
|
|||