| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.76 - 3.80 g/cc | 0.136 - 0.137 lb/in³ | Sintered |
|
Nabaltec GRANALOX® NM 9622 B Ceramic Body, Binder Free
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casti..
|
|||
| Density | 3.76 g/cc | 0.136 lb/in³ | |
|
Ferro EG 2807 Metal Sealing
Glass Type: Zn-B-Si (devit) Typical Powder Form: VSD Typical Application: Kovar Mo, W Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matc..
|
|||
| Density | 3.77 g/cc | 0.136 lb/in³ | |
|
Schott N-LAK22 Glass
Information Provided by SCHOTT North America, Inc.
|
|||