| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 9.20 g/cc | 0.332 lb/in³ | |
|
Indium Corp. Indalloy 78 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
|
|||
| Density | 9.19 g/cc | 0.332 lb/in³ | |
|
Indium Corp. Indalloy 80 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
|
|||
| Density | 9.20 g/cc | 0.332 lb/in³ | |
|
Lucas-Milhaupt BRAZE 452
Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap ..
|
|||
| Density | 9.19 g/cc | 0.332 lb/in³ | |
|
Indium Corp. Indalloy 216 Silver Solder Alloy
Information Provided by Indium Corporation
|
|||
| Density | 9.18 g/cc | 0.332 lb/in³ | |
|
Lucas-Milhaupt EASY FLO 35 Silver Based Cadmium-Bearing Filler Metal
Applications: Easy-Flo 35 is a are good general purpose, low temperature silver brazing filler metals for joining both ferrous and nonferrous metals. Because of their fairly low cost, good fatigue ..
|
|||