| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.899 g/cc | 0.0325 lb/in³ | Injection molded specimen; ASTM D1505 |
|
Phillips Sumika Marlex® CHP-035 Thermoplastic Polyolefin
(discontinued **)
Applications: Painted air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
|
|||
| Density |
0.899
g/cc @Temperature 20.0 °C |
0.0325
lb/in³ @Temperature 68.0 °F |
|
|
LyondellBasell PE Propylene glycol ethyl ether
Information provided by Lyondell.
|
|||
| Density | 0.899 g/cc | 0.0325 lb/in³ | ASTM D1475 |
|
Humiseal 1A20LSE Urethane Conformal Coating
Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther..
|
|||
| Density | 0.899 g/cc | 0.0325 lb/in³ | ASTM D1475 |
|
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
|
|||
| Density | 0.899 g/cc | 0.0325 lb/in³ | ASTM D1475 |
|
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..
|
|||
| Density | 0.899 - 1.02 g/cc | 0.0325 - 0.0368 lb/in³ | |
|
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series
|
|||
| Density | 0.899 - 0.923 g/cc | 0.0325 - 0.0333 lb/in³ | |
|
Lord Adhesives 7701 Ethyl Acetate Surface Conditioner
Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa..
|
|||
| Density |
0.899
g/cc @Temperature 15.6 °C |
0.0325
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil Mobil Almo 527
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
|
|||
| Density |
0.899
g/cc @Temperature 15.0 °C |
0.0325
lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
|
ExxonMobil 60 Mobilube XFD
Mobilube XFD 50 and 60 are extra high performance drivetrain lubricants engineered specifically to provide optimum component life when used as recommended in Caterpillar final drives and axles. Th..
|
|||
| Density |
0.899
g/cc @Temperature 15.6 °C |
0.0325
lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
|
ExxonMobil Mobil Almo 527
Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio..
|
|||
| Density |
0.899
g/cc @Temperature 15.0 °C |
0.0325
lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
|
ExxonMobil 60 Mobilube XFD
Mobilube XFD 50 and 60 are extra high performance drivetrain lubricants engineered specifically to provide optimum component life when used as recommended in Caterpillar final drives and axles. Th..
|
|||
| Density | 0.899 g/cc | 0.0325 lb/in³ | Injection molded specimen; ASTM D1505 |
|
Phillips Sumika Marlex® ABF-035 Thermoplastic Polyolefin
(discontinued **)
Applications: Vehicle front-end air damsHigh impact exterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This produc..
|
|||