| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Polymer Industries Densetec HDPE Cutting Board Densetec Cutting Board is engineered for durability, low maintenance and safety. Its textured, matte surface safely holds food in place without slipping. The "natural" bright white color is favored .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Polymer Industries Densetec HDPE Partition Board Polymer Industries Densetec High Density Polyethylene Partition Board is the ideal partition material for a wide variety of commercial applications such as schools, parks, stadiums, office buildings.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | |
| Reltek BONDiT™ HM-502 Coating, Sealant, Adhesive System A protective coat for most metal, glass, and ceramic materials for use against corrosion and other chemical attacks. Useful against fungi growth. Bondit HM-502 is a thermoplastic emulsion system.Inf.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Petromont 1002 High Density Polyethylene Resin Petromont HDPE 1002 is a blow moulding high-density polyethylene copolymer resin produced using the UNIPOL® Process. This multi-purpose resin can be used on intermittent and continuous extrusion bl.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Polikim ULPOLEN® 1000 UHMWPE, Oil The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer
(discontinued **) High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat
(discontinued ** High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Braskem BT 100K HDPE Blow Molding Polyethylene
(discontinued **) Applications: Large containers from 60 to 200 litersInformation provided by Braskem |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Global B-8200 High Density Polyethylene Description-high molecular weight, excellent stress cracking resistance,
excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| Ineos B53-35H-011 HDPE Ineos B53-35H-011 is a high density polyethylene copolymer developed for blow molding applications. This product is recommended for use in applications which require a combination of high top load .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| Ineos B53-35H-100 HDPE B53-35H-100 is a high density polyethylene copolymer developed for injection blow molding. Zinc Stearate is incorporated in the formulation as a release agent. It is recommended for use in applica.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D4883 |
| Ineos K44-15-123 HDPE Copolymer with Carbon Black Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO R 1183 |
| Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D792 |
| Solvay Specialty Polymers Polidan® TUX 100 Polyethylene, Crosslinked (XLPE) Polidan® TUX 100 is a high density crosslinkable polyethylene compound manufactured according to the Sioplas® process. It has been developed for the production of crosslinked pipes in a wide r.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1872/1 |
| SIDPEC EGYPTENE® HD 5403 EA HDPE Blow Molding Applications:Blow molded containers up to 30 liters for packagingChemicalsHousehold productsOils and foodstuffsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemi.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Borealis BorPURE™ MB6562 High Density Polyethylene for Injection Molding BorPure™ MB6562 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Formosa Plastics Formolene® HB5502A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5502A is designed for applications requiring excellent stiffness and stress crack resistance properties. It.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Formosa Plastics Formolene® HB5502Z Blow Molding HDPE Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502Z eliminates the need for including a mold release agent at each machine, by incorporating zinc stearate w.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Borealis BorPURE™ MB6561 High Density Polyethylene for Injection Molding BorPure™ MB6561 is a bimodal, high-density polyethylene intended for injection and compression molding. This grade combines excellent organoleptic properties, environmental stress crack resistance .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Total HP 401 MDPE, pipe, cable, sheet FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Formosa Plastics Formolene® HB5502B Blow Molding HDPE Hexene CopolymerApplications: Injection blow molded pharmaceutical packagingFormolene HB5502B is designed for applications requiring excellent stiffness and stress crack resistance properties. It ma.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ExxonMobil Method |
| ExxonMobil Escorene® UL 7840E Adhesive Application Resin Escorene Ultra UL 7840E is a 31.4% vinyl acetate copolymer that has good compatibility with both hydrocarbon and natural tackifiers and is suitable for making hot melt adhesives adn sealants. UL 784.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ISO 1183 |
| Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Amco PRIMATOP HDPE 003955BAS Hexene Copolymer HDPE 003955BAS features excellent stiffness, stress crack resistance properties, and antistat. Applications include blow molding and sheet extrusion thermoforming.Former A-Top Polymers product; part.. |
|||
| Density | 0.955 g/cc | 0.0345 lb/in³ | ASTM D1505 |
| Chevron Phillips Marlex® HMN 55180 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520. Excellent impact strength and warpage resistance; high surface gloss.Data provided by the manufacturer |
|||