Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Quadrant EPP Cestilene™ HD 500 R Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
SABIC M40060 Series High Density Polyethylene for Injection Molding
Product Description: M40060 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid..
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183
Polykemi AB POLYfill PPH GF5010 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Heat Resistant
Information provided by Polykemi AB
Density 0.960 g/cc
0.0347 lb/in³
Finaprene 2602 Method
Total Finaprene® 602 Thermoplastic Elastomer  (discontinued **)
Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Thanks to is broad molecular weight distribution, Finaprene® 602 provides good fluidity properties..
Density 0.960 g/cc
0.0347 lb/in³
Finaprene 2602 Method
Total Finaprene® 602D Clear Impact Polystyrene  (discontinued **)
Finaprene® 602D is a clear high styrenic styrene-butadiene (SBS) block copolymer with a radial structure, which is widely used as modifiers or in alloys with many plastic resins, such polystyrene, ..
Density >= 0.960 g/cc
>= 0.0347 lb/in³
ASTM D1505
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
NOVA Chemicals Sclair® 59F HDPE Blow Molding Resin  (discontinued **)
Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer.
Density 0.960 - 1.30 g/cc
0.0347 - 0.0470 lb/in³
Average value: 1.05 g/cc Grade Count:13
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
LyondellBasell Alathon® M6020 High Density Polyethylene
ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typica..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D3574A
Mearthane Durethaneâ„¢ F DF-245A Closed Cell Foam Polyurethane
TDI backbone: ester.Shore 00 Hardness: 90Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient..
Density >= 0.960 g/cc
>= 0.0347 lb/in³
Mikro-Technik Mikrolen AST UHMW-PE
Antistatic ModifiedProperties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at ..
Density 0.960 g/cc
0.0347 lb/in³
Silon Taborex TA 2111 HD Catalyst Masterbatch
Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1108 HD, TA 1109 HD. TA 2111 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a S..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP
LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Density 0.960 - 1.04 g/cc
0.0347 - 0.0376 lb/in³
RP-0549
Solvay RHODATERGE® MULTIGREEN II Surfactant
Description: Rhodaterge® Rhodaterge® Multigreen II is a general purpose Green Concentrate. It provides excellent oily soil removal for household, industrial and institutional products. It sis ..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Westlake Plastics Propylux® CN-P Polypropylene (conductive)
Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio..
Density 0.960 g/cc
0.0347 lb/in³
Goodfellow Polyethylene Fiber/Polyethylene composite
Information provided by Goodfellow.
Density 0.960 g/cc
0.0347 lb/in³
Zircar Ceramics RAHP Reticulated Alumina Hearth Post
ZIRCAR Reticulated Alumina Hearth Posts are rigid highly porous rods and shapes of fine grain dense alumina ceramic. An off-shoot of superalloy casting technology from the aerospace industry, these ..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792, ISO 1183
DuPont™ HPF® 1000 Amorphous Polymer for Golf Balls
DuPont™ HPF 1000 is extremely versatile and can be used to manufacture all layers of golf balls. DuPont™ HPF 1000 offers a combination of high resilience and low compression. This polymer is a hig..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Aclo Accutech Polypropylene Homopolymer HP0334G10CL Glass Reinforced Coupled
Density 0.960 g/cc
0.0347 lb/in³
ASTM-D792
Braskem IA59U3 HDPE Injection Molding Polyethylene Homopolymer
IA59U3 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high stiffness and impact strength combined ..
Density 0.960 g/cc
0.0347 lb/in³
BASF DiethylenetriaminE
Formula: C4H13N3CAS: 111-40-0Description: Diethylenetriamine is a colorless to yellow liquid with an amine-like odor.Synonyms: DETA, Bis(2-aminoethyl)amine, 1,4,7-Triazaheptane, 1,5-Diamino-3-azapen..
Density 0.960 g/cc
0.0347 lb/in³
ISO 2781
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Amco PRIMATOP HDPE RP 004 Granular High Density Polyethylene
HDPE RP 004 features small particle size and is used in plastic lumber extrusion.Former A-Top Polymers product; part of Amco product line since 2013.
Density 0.960 g/cc
<br>@Temperature 23.0 °C
0.0347 lb/in³
<br>@Temperature 73.4 °F
ISO 1183
Arkema Group EVATANE® 33-400 Copolymer Ethylene - Vinyl Acetate
EVATANE® 33-400 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-400 is stabilized with antioxidants. The High Vinyl Acetate ..
Density 0.960 g/cc
0.0347 lb/in³
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry)
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin &nbsp;(discontinued **)
Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer.
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin
Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc..