| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
SABIC M80064 Series High Density Polyethylene for Injection Molding
Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D 792 |
|
NOVA Chemicals Sclair® IG464-C Compression Molded HDPE Resin
IG464-C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG464..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | Exxon Method |
|
ExxonMobil Iotek® 7610 Zinc Ionomer
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low melt index zinc ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact streng..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
ICO Polymers ICOFLOâ„¢ 510-5008 1200 Micron HDPE Powder
Description: ICOFLO 510-5008 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D792 |
|
IRPC Polimaxx Polene GM2865 High Density Polyethylene
CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | |
|
JPJ Technologies 1500J HDPE Injection
Information provided by JPJ Technologies
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | |
|
JPJ Technologies 2200J HDPE Injection
Information provided by JPJ Technologies
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ISO 1183 |
|
Borealis MG9641B Polyethylene
MG9641B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ISO 1183 |
|
Borealis MG9641S Polyethylene
MG9641S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ISO 1183 |
|
Borealis MG9647B Polyethylene
MG9647B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Formosa Plastics Formolene® HB6007 Blow Molding HDPE
HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excell..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Formosa Plastics Formolene® HP6000 Pipe HDPE
High Density Polyethylene Homopolymer for Pipe Extrusion Formolene® HP6000 is a high quality product for homopolymer pipe extrusion applications. It has excellent stiffness and good stiffness prope..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene
High Density PolyethyleneCustomer Benefits: A blow molding grade rein that offers a high quality product for those critical food packaging jobs and good impact strength and stiffness.Applications: L..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Chevron Phillips Marlex® K606 High Density Polyethylene
High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D4883 |
|
ExxonMobil HDPE HMA 025 High Density Polyethylene Resin
Product Description: HMA 025 is a HDPE grade, characterized by excellent dimensional stability, impact strength and very high stiffness. Availability: Africa & Middle East, Asia Pacific and Europe A..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D4883 |
|
ExxonMobil HDPE HMA 035 High Density Polyethylene Resin
Product Description: HMA 035 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, good impact strength and very high stiffness. Availability: Africa & Middle East, Asia ..
|
|||
| Density | 0.964 - 0.969 g/cc | 0.0348 - 0.0350 lb/in³ | ASTM D4052 |
|
ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaInformation provided by ExxonMobil
|
|||
| Density | 0.964 - 0.968 g/cc | 0.0348 - 0.0350 lb/in³ | ASTM D4052 |
|
ExxonMobil Jayflex™ DIDP Plasticizer (European Grade)
Availability: Europe, Middle East & AfricaCAS Number: 68515-49-1EC Number: 271-091-4Information provided by ExxonMobil
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D792 |
|
Entec Hypel® PEHD10/.964 HDPE
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ExxonMobil Method |
|
ExxonMobil HD 7925.30 Barrier Film Resin
Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Chevron Phillips Marlex® K607 High Density Polyethylene
(discontinued **)
High Density PolyethyleneCustomer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.Applications: Recommended resin for thin sheet, cut sheet up to..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D1505 |
|
Amco PRIMATOP HDPE 006964 Blow Molding Polyethylene
HDPE 004955HP features excellent stiffness to ESCR ratio and good impact resistance. Applications include oil bottles, household and industrial chemical containers, and personal care products.Former..
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | ASTM D792 |
|
Micropol Isoplas P602 Crosslinkable Polyethylene
Information provided by Micropol Limited
|
|||
| Density | 0.964 g/cc | 0.0348 lb/in³ | Exxon Method |
|
ExxonMobil Iotek® 7030 Zinc Ionomer Molding/Extrusion Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas..
|
|||