Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.970 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
TPE-0105 (ASTM D792)
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber  (discontinued **)
A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc..
Density 0.970 g/cc
0.0350 lb/in³
Melt
Covestro Apec® DP 1-9379/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792 - ISO 1183
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792 - ISO 1183
DuPont Bexloy® AXW504BK Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Density 0.970 g/cc
0.0350 lb/in³
Honeywell Spectra® 900 Fiber
Spectra® fiber 900 was the first commercially available extended-chain, high-strength polyethylene fiber and the first in a series of Spectra® fibers. Spectra® fiber has one of the highest ..
Density 0.970 g/cc
0.0350 lb/in³
Not Compounded
KKPC KOSYN 1721 Styrene Butadiene Rubber
Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and..
Density 0.970 g/cc
0.0350 lb/in³
LATI Latiblend 5262 PP Homopolymer/PA6
Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP
SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS..
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Techmer ES Luriblend® PE 5902
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP MX88028 PP
LNP* THERMOCOMP* MX88028 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Washington Penn Medium Impact Copolymer 10% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Density 0.970 g/cc
0.0350 lb/in³
Dow Corning SYL-OFF® PMCPSL 800 Coating
Suitable for lamination with a variety of adhesives, maleate-inhibited coating offers improved thin film stability vs. conventional release coatings and excellent anchorage stability with super cale..
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792, ISO 1183
DuPont™ Entira® AS MK 400 Ionomer Resin
Entira™ AS MK400 is an extremely hygroscopic ionomer resin that is supplied as free-flowing pellets.
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
DuPont™ Surlyn® 9120 Ionomer Resin, Zinc
Surlyn® 9120 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr..
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Diamond Polymers Softflex® 2701-1502R
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Diamond Polymers Softflex® 8200
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 0.970 g/cc
0.0350 lb/in³
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Density 0.970 g/cc
0.0350 lb/in³
DIN 53479
Dynasol Solprene® 303 Random-Block Copolymer
Solprene 303 is a linear random-block styrene-butadiene copolymer with 46% styrene content, 11% present as a polystyrene block. S-303 is used in vulcanized microcellular shoe soles, it provides hard..
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Density 0.970 g/cc
0.0350 lb/in³
Arkema Group Evatane® 1005 VL 2C Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for thermal agricultural films to 180 at 200 µ with diffusing effect, for greenhouse coverage.ISO d..
Density 0.970 - 0.976 g/cc
0.0350 - 0.0353 lb/in³
ASTM D4052
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792 - ISO 1183
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Copyright © lookpolymers.com All Rights Reserved