| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density |
1.10
-
1.10
g/cc @Temperature 325 - 325 °C |
0.0397
-
0.0397
lb/in³ @Temperature 617 - 617 °F |
Average value: 1.10 g/cc Grade Count:1 |
|
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Density | 0.00310 - 1.10 g/cc | 0.000112 - 0.0397 lb/in³ | Average value: 0.108 g/cc Grade Count:273 |
|
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
|
|||
| Density | 0.980 - 1.10 g/cc | 0.0354 - 0.0397 lb/in³ | Average value: 1.04 g/cc Grade Count:84 |
|
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..
|
|||
| Density | 0.700 - 1.10 g/cc | 0.0253 - 0.0397 lb/in³ | ASTM B212 |
|
H.C. Starck Amperit® 847.6 Agglomerated Yttria (Y2O3) |
|||
| Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | 5% Lucobit in Bitumen B50/70 |
|
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen
Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures ..
|
|||
| Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | 2.4% Lucolast in Bitumen B50/70 |
|
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive
Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit..
|
|||
| Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | |
|
Solvay GEROPON® TK 32 Surfactant
Description: GEROPON TK-32 is an effective dispersant in liquid formulationsChemical Name: SODIUM N-METHYL-N-TALL OIL TAURATECAS: 61791-41-1, 67-63-0Solubility in water: SolubleAvailable in: Asia Pa..
|
|||
| Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | |
|
Solvay MIRACARE® SLB-205/N Surfactant
Description: Miracare SLB-205/N is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a ..
|
|||
| Density | 1.00 - 1.10 g/cc | 0.0361 - 0.0397 lb/in³ | RP-17617 |
|
Solvay MIRACARE® SLB-365/G Surfactant
Description: Miracare® SLB-365/G is a complete formulated system containing mild anionic and amphoteric foaming surfactants and a structuring agent in an easy to use lamellar concentrate. Upon di..
|
|||
| Density | 1.06 - 1.10 g/cc | 0.0383 - 0.0397 lb/in³ | AV15 |
|
Solvay Amyl Acid Phosphate
Identification: AMYL ACID PHOSPHATE - Phosphoric acid, mono – and bis –(branched and linear pentyl esters)CAS: 84418 – 71 – 3Available in: Asia Pacific, Europe, Latin America and..
|
|||
| Density | 0.0280 - 1.10 g/cc | 0.00101 - 0.0397 lb/in³ | Average value: 0.876 g/cc Grade Count:36 |
|
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
|
|||
| Density | 1.06 - 1.10 g/cc | 0.0383 - 0.0397 lb/in³ | Average value: 1.07 g/cc Grade Count:9 |
|
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend". Each property range of values reported is minimum and ma..
|
|||
| Density |
1.10
-
1.10
g/cc @Temperature 325 - 325 °C |
0.0397
-
0.0397
lb/in³ @Temperature 617 - 617 °F |
Average value: 1.10 g/cc Grade Count:1 |
|
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
|
|||
| Density | 0.947 - 1.10 g/cc | 0.0342 - 0.0397 lb/in³ | Average value: 1.00 g/cc Grade Count:18 |
|
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
|
|||