| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Nylene® 615 Nylon 6, Film Grade
Film Grade. Nylene 615 is an extrusion grade nylon 6 resin suitable for coating and film co-extrusion applications. It has excellent melt stability and good melt strength. Nylene 615 has superior
..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermedia..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | Dry As Molded |
|
Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned
(discontinued **)
Standard injection molding grade, easy flow, easy mold release, fast setting.Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric...
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH GF10030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Density |
1.12
-
1.12
g/cc @Temperature >=250 °C |
0.0405
-
0.0405
lb/in³ @Temperature >=482 °F |
Average value: 1.12 g/cc Grade Count:1 |
|
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | DIN 53479; ASTM D792 |
|
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
Taiwan Sheen Soon Sheenthane® A8960N Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM Data |
|
Styron Pulse® 600 ABS + Polycarbonate
PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® HDPE TM20 UV BK 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: BlackInformation provided by TP Composi..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
|
|||
| Density |
1.12
g/cc @Temperature 25.0 °C |
0.0405
lb/in³ @Temperature 77.0 °F |
|
|
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Aclo Accutech Polypropylene Homopolymer HP0334G15M15CL Glass/Mineral Reinforced Coupled |
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Aclo Accutech Polypropylene HP0335G30CHIV Homopolymer Glass Reinforced High Impact Coupled
Approved to GMP.PP.017 Black A12563
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
BASF Procom® GC30H 251 Polypropylene
Uses: car and truck fans and shrouds, car rear light housings, car radiator expansion tanks, car grills, domestic appliance components (e.g. washing machine tanks, impellers housings, etc.), textile..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
BASF Procom® GC30S 403 Polypropylene
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
|
|||
| Density | 1.12 - 1.15 g/cc | 0.0405 - 0.0415 lb/in³ | ISO 1183 |
|
BASF Ultramid® B40 PA6
Description: Ultramid® B40 is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round pellets.Infor..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
BASF Ultramid® C40 01 PA66/6 (Dry)
Ultramid C40 01 is a high viscosity, copolymer PA6/66 grade. Its very low melting point compared to standard PA6 is advantageous for coextrusion with temperature sensitive polymers like EVOH. It c..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
A.D. Compound Adene NTJA Homopolymer 30% Talc Filled Polypropylene
Information provided by A.D. Compound
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ISO 1183 |
|
BASF Ultramid® C33 PA6/66
Description: Ultramid® C33 is a copolyamide 6/66 grade of intermediate viscosity for the production of mulitlayer film and monofilaments. Ultramid® C33 is well suited for the production of nonsymm..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | ASTM D792 |
|
Chem Polymer Chemlon 223 Nylon 6, Nucleated
A highly nucleated, lubricated nylon 6 intended for applications requiring a faster cycle time. It has increased tensile strength, rigidity, creep resistance and hardness over general purpose nylon..
|
|||
| Density |
1.12
g/cc @Thickness 2.00 mm |
0.0405
lb/in³ @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D792 |
|
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer
Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation.
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | |
|
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, General Description
(discontinu
Product form is white, odorless chips. Distinguishing Feature: Readily soluble in common solvents. Good low temperature flexibility.29 % Chlorine Content. 1.4% Sulfur Content. Very Good Abrasion..
|
|||
| Density | 1.12 g/cc | 0.0405 lb/in³ | Latex |
|
DuPont Performance Polymers AquaStik® AQS-2161 Polychloroprene Latex
(discontinued **)