Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
NYCOA 2025 Nylon 6
extrusion and molding grade with mold release and quicker cycle times for sports cleatsInformation provided by NYCOA, Inc.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Nylene® 402 Nylon 6
Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant
Information provided by Polykemi AB
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Density 1.13 - 1.14 g/cc
0.0408 - 0.0412 lb/in³
Average value: 1.14 g/cc Grade Count:10
Overview of materials for Nylon 6 Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6 Fiber". Each property range of values reported is minimum and maximum values of appropriate MatW..
Density 1.13 - 1.20 g/cc
0.0408 - 0.0434 lb/in³
265 Resin
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive
LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Mitsubishi Xantar® C CM 406 FD Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Density 1.13 g/cc
0.0408 lb/in³
ISO R 1183
Schwartz Technical Plastics LAMIGAMID® 307 Cast Polyamide 6, Heat Stabilized, Conditioned
Application: slippers, inserts for coupling boxesInformation provided by Schwartz Technical Plastics GmbH
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Techmer ES HiFill® PA6 L LE MB
Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp MFM43S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MFM43S is a compound based on Polypropylene resin containing Glass Fiber, Mineral. Added features include : Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183-87
Wellman Wellamid® 42L-N Nylon 6, General Purpose
All information provided by Wellman Engineered Resins.
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber
30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D 792
Cossa Polimeri ESTABLEND 6500 A Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 HWCP Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
Density 1.13 g/cc
<br>@Temperature 25.0 °C
0.0408 lb/in³
<br>@Temperature 77.0 °F
DSM Somos® 9420 Epoxy Resin for Stereolithography
DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid..
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Diamond Polymers NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded
Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar.
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Aclo Accutech Polypropylene Copolymer CP0437T30L Talc Reinforced
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Aclo Accutech Polypropylene Copolymer CP0437W30L1 Wollastonite Reinforced
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Ashley Polymers Ashlene® 539 Nylon 66
Extrusion grade for film & monofilament.Data provided by the manufacturer
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Polykemi AB POLYfill PPHC T11030 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Ashley Polymers Ashlene® PC/ABS Alloy
Flame retardant alloy.Data provided by the manufacturer
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Ashley Polymers Ashlene® R6020 Nylon 6
A medium viscosity extrusion grade resin with excellent melt stability and good melt strength, suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughn..
Density 1.13 g/cc
0.0408 lb/in³
Latex
DuPont Performance Polymers Neoprene 671A Polychloroprene &nbsp;(discontinued **)
Main feature: DPHS. Principal uses include: Dipped goods, Coatings, Mastics, Thread, Adhesives (Lamination, Contact).Solids content: 59%. Initial pH: 12.5. Surface tension: 41 dyne/cm. Polymer t..