| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | |
|
Nylene® PA6/6 Homopolymer 132 HSL Nylon 6/6
Low Viscosity GP Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | |
|
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer
High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
PTS Trimid® N6-600 Medium Viscosity Extrusion Grade Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Density | 1.14 - 1.60 g/cc | 0.0412 - 0.0578 lb/in³ | Average value: 1.28 g/cc Grade Count:250 |
|
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | DIN 53479; ASTM D792 |
|
Kolon KOPA® KN333HRN Heat Resistant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | Test Method A; ISO 1183:1987 |
|
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 402 Natural FA PA66, DRY
Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRILOY U2000A PPA (Asia Pacific)
LNP* Lubriloy* U2000A is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 E4 HS MB Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat Stabilized and High ViscosityInformation provided by TP Composites, Inc.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, Conditioned
Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | DIN 53479 |
|
Polyram PlusTek RA601 Nylon 6.6, Heat Resistant
Heat resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified
Impact modified Nylon 6 for injection molding applications.Information provided by Polyram.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | (DAM); ISO 1183 |
|
DSM Akulon® S223-DK Nylon 66 (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | (DAM); ISO 1183 |
|
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
DSM Akulon® S223-F Nylon 66 (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
Diapolyacrylate Shinko-Lac® U400B Transparent ABS
Shinko-Lac® is a registered trademark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Eurostar Star C BX6088 ABS, 20% Carbon Filled, Injection Molding
Star C BX06008 is a 20% Carbon Fiber Reinforced ABS Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding
Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Arkema Group Pebax® MH 1657 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MH 1657 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MH 1657 is an inherently dissipative polymer and can be dry blended or compounded w..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
Aclo Accutech Polypropylene Homopolymer HP0336T30L Talc Reinforced |
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D-792 |
|
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy
ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali
|
|||
| Density | 1.14 - 1.19 g/cc | 0.0412 - 0.0430 lb/in³ | Part A |
|
3M Scotch-Weld™ DP601 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
|
Aclo Accutech SAN SAN930G10L Glass Reinforced |
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Borealis Xmod™ K65G3 30% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G3 is a 30% glass fiber reinforced grade intended for injection molding. Xmod K65G3 has been developed especially for the car industry, to be used UTB parts. Xmod K65G3 offers good balance..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
|
Mitsubishi Xantar® C CM 506 Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
|
|||
| Density | 1.14 g/cc | 0.0412 lb/in³ | |
|
3M Novec™ 4200 Electronic Surfactant
3M™ Novec™ 4200 Electronic Surfactant is an anionic fluorochemical surfactant in a 25% aqueous solution with low metal content, typically < 500 ppb of each specified metal. Novec 4200 surfactant p..
|
|||