Polymer Property : Density = 1.20 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® AD4820 PC
LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® CFR7630 PC COPOLYMER
Lexan* CFR7630 Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm ..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER
Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. ..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific)
UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East)
Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific)
PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
SABIC Innovative Plastics LNP COLORCOMP D1000P PC
LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing.
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape  (discontinued **)
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu..
Density 1.20 g/cc
0.0434 lb/in³
ISO 2781
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane
Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling ..
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade
High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mitsubishi Xantar® MX 2042 FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRILOY D20001 PC (Asia Pacific)
LNP LUBRILOY* D20001 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant.
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Shuman 910 Utility Black Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A; ASTM D792
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
Density 1.20 g/cc
0.0434 lb/in³
ASTM Data
Styron CALIBREâ„¢ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant
CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g..
Density 1.20 - 1.50 g/cc
0.0434 - 0.0542 lb/in³
ASTM D792
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy
EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl..
Density 1.20 g/cc
0.0434 lb/in³
Saint-Gobain Chemfab® 14 Porous PTFE-Coated Glass
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183-1
Covestro Makrolon® 2405 MAS048 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 GV 10 HWCP 10% Glass Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.20 g/cc
0.0434 lb/in³
Arlon SQA-TMS-024
Arlon RBLW401X##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Rubber
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths. ## in the product number indicates roll length in yards..
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Ashley Polymers Ashlene® 1051 Polycarbonate
A general purpose injection molding grade, natural resin. Also available as: 1051R (with release), 1053 (with UV stabilizers), 1053R (with release and UV stabilizers).Data provided by the manufactu..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Covestro Makrolon® LQ2687 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9MVR (300 °C/1.2 kg) 12.5 cm3/10 minOptical lensMedium viscosityUV stabilizedUV 400 cut offEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear t..
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
CENTROPLAST CENTROCARB Polycarbonate
CENTROCARB is a transparent or semi-transparent plastic with high strength and impact resistance. It is dimensionally rigid and has very good electrical insulating properties. It is used in contain..
Density 1.20 g/cc
0.0434 lb/in³
ASTM A792
PlastxWorld Veroplas PA2001F Nylon 6
flame retarded (UL94 VO), unfilled injection molding gradeInformation provided by PlastxWorld Inc.