Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.23 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre
FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.23 - 1.73 g/cc
0.0444 - 0.0625 lb/in³
Average value: 1.45 g/cc Grade Count:117
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Density 1.23 - 1.26 g/cc
0.0444 - 0.0455 lb/in³
322 Hardener
Lord Adhesives 320 / 322 Epoxy Adhesive
LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides ..
Density 1.23 g/cc
0.0444 lb/in³
LATI Laticonther 52/35 CP1/45 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation ..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF13 L 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Comp..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
Density 1.23 g/cc
0.0444 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon DE002P PC (Asia Pacific)
LNP STAT-KON* DE002P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Techmer ES HiFill FR® PA6 GF13 FR-N IM BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilize, Impact Modifier and LubricantFeatures: Flame Retardant, Heat S..
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
TPI Porene® ABS-AN450 Flame Retardant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183-87
Wellman Wellamid® GFT1835-WBK1 Nylon 66, 17% Glass Fiber Reinforced, Impact Modified
All information provided by Wellman Engineered Resins.
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Eurostar Star L PA66 D51 PA66, Injection Molded
Star L PA66 D51 is a PTFE Lubricated, Unreinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural
Information provided by Eurotec®
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Density 1.23 g/cc
0.0444 lb/in³
BASF Lupranate® M20HB Isocyanate
Description: Lupranate® M20HB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20HB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer
Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Ashley Polymers Ashlene® 520S-13GU Nylon 66, 13% Glass Reinforced
Nylon 66, 13% Glass reinforced resin with heat stabilizer, utility grade. Also available in black (520S-13GBU).Data provided by the manufacturer
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183-1-A
BASF Elastollan C 85 A HPM TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c..
Density 1.23 g/cc
0.0444 lb/in³
BASF Lupranate® 274 Isocyanate
Description: Lupranate® 274 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate 274 Isocyanate is suitable for the production of rigid insulation foams by molding, sp..
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792-91
Multibase Multi-ABS 3245 FR Flame Retardant ABS
Data provided by Multibase.
Density 1.23 g/cc
0.0444 lb/in³
DuPont Performance Polymers Neoprene AD-5 Polychloroprene Rubber  (discontinued **)
Description: Chloroprene polymer designed for use in high strength solution adhesives requiring rapid rates of strength development. More color-stable than neoprene AC during storage.Processing and ..
Density 1.23 - 1.27 g/cc
0.0444 - 0.0459 lb/in³
ISO R 1183
Fainplast Compounds PMP 57 Flexible PVC, Extrusion Modified with PU
Profiles mixed rubber/PU
Copyright © lookpolymers.com All Rights Reserved