Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Multibase Multi-Pro® 4012 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo..
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Polykemi AB SCANTEC PC S75FR Polycarbonate
Information provided by Polykemi AB
Density 1.24 g/cc
0.0448 lb/in³
TPE-0105 (ASTM D792)
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber  (discontinued **)
A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b..
Density 1.24 - 1.29 g/cc
<br>@Temperature 250 - 295 °C
0.0448 - 0.0466 lb/in³
<br>@Temperature 482 - 563 °F
Average value: 1.26 g/cc Grade Count:7
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Density 1.24 g/cc
0.0448 lb/in³
Idemitsu Kosan Xarec® D132 SPS, 25% Glass Filled
Density 1.24 g/cc
0.0448 lb/in³
Taiwan Sheen Soon Sheenthane® D7620 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DE003ER PC
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP HB006 PA11
LNP* Thermocomp* HB006 is a compound based on Nylon 11 resin containing 30% Glass Bead.
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific)
LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific)
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL GTX GTX679 PPE+PA6
Noryl GTX* GTX679 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to al..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Washington Penn PPUP4G402 Polypropylene, 40% Talc Filled, High Flow
Exceptional retention of mechanical properties and appearance upon long term heat aging.Applications: Appliance parts.Data provided by Washington Penn Plastic Co., Inc.
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479
Polyram RamTough PZ300G3 Polycarbonate, 15% Glass Fiber
15% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Covestro Bayblend® T95 MF* Polycarbonate + ABS, Mineral Filled
Developmental productInjection molding grade9 % mineral filledvery high heat resistancereduced coefficient of linear thermal expansiontensile modulus = 3350 MPaVicat/B 120 = 142 °CPreprocessingMax...
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T..
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of..
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us..
Density 1.24 g/cc
0.0448 lb/in³
Arkema Group Rilsan® BUM 30 Nylon 11, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High comp..
Density 1.24 g/cc
0.0448 lb/in³
Side 2, Silicone Property; Arlon SQA-TMS-024
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer
Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fue..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated
A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general pu..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Plastics Group Polifil® RMT-40V 40% Talc-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMT-V series compounds are high impact, UV stabilized polypropylenes reinforced with asbestos-free talc. In addition to high impact strength, they possess a high flex modulus and the abili..
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade &nbsp;(discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it ..
Density 1.24 - 1.28 g/cc
0.0448 - 0.0462 lb/in³
ISO R 1183
Fainplast Compounds PG 6620 Flexible PVC, Extrusion Modified with Rubber
Profiles modified with rubber
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Buckeye Polymers BP RPP 4012 TU Polypropylene, 40% Mineral Filled
UV StabilizedThis Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistan..