Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Multibase Multi-Pro® 4010 M Polypropylene
Mica Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses:Pump PartsInformation provided by Multibase
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East)
Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes..
Density 1.25 g/cc
0.0452 lb/in³
Pyrotek R-3 Braided Glass Rope
Dense, solid, square braided glass rope. Good where physical abuse and abrasion are a problem.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek.
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Polykemi AB POLYshine PBT D241 PBT, Impact Modified
Information provided by Polykemi AB
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Ravago Manufacturing Americas Hybrid B6720U Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Density 1.25 g/cc
0.0452 lb/in³
ASTM Data
Dow Questra® WA550 High Heat Syndiotactic Polystyrene, 30% Glass Filled  (discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Density 1.25 - 1.68 g/cc
0.0452 - 0.0607 lb/in³
Average value: 1.53 g/cc Grade Count:41
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East)
LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance.
Density 1.25 - 1.56 g/cc
0.0452 - 0.0564 lb/in³
Average value: 1.41 g/cc Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Density 1.25 g/cc
0.0452 lb/in³
LATI Latilub 52/30-15T G/30 PP Homopolymer, 30% Glass Fiber Reinforced
Self-lubricating product based on Polypropylene homopolymer (PPh). PTFE. Glass fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DX07404H PC
LNP* LUBRICOMP* DX07404H is a compound based on Polycarbonate containing Proprietary Fillers. Added features of this grade are: Healthcare, Wear Resistant.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites..
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Techmer ES Statiblend® PA6 02012
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318TPCI# 1038102Information provided by TP Composites, Inc.
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Stir SpA T 5599 A (PVC)
Application: Non-toxic transparent pipe for conveying waterInformation provided by STIR SpA
Density 1.25 g/cc
0.0452 lb/in³
DIN 53479
Polyram PlusTek PD300G4 Nylon 12, 20% Glass Fiber
20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System
0.1 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and offi..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
DSM Akulon® S223-G2U (Dry) 13% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 CF 18 HWCP 18% Carbon Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.25 - 1.29 g/cc
0.0452 - 0.0466 lb/in³
ISO R 1183
Fainplast Compounds GS 6020 Flexible PVC, Injection Molding for Footwear
High boots
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness
Data provided by Adell Plastics, Inc.
Density 1.25 g/cc
0.0452 lb/in³
ISO R1183
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Beijing Chemical Industry KAIFA® M109-G20N MPPO Resin
20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber  (discontinued **)
Data provided by PolyOne.
Density 1.25 g/cc
0.0452 lb/in³
Loctite® 549 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..