| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.910 - 1.28 g/cc | 0.0329 - 0.0462 lb/in³ | Average value: 1.07 g/cc Grade Count:3 |
|
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Density | 0.775 - 1.28 g/cc | 0.0280 - 0.0462 lb/in³ | Average value: 1.06 g/cc Grade Count:25 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..
|
|||
| Density |
1.27
-
1.28
g/cc @Temperature 295 - 295 °C |
0.0459
-
0.0462
lb/in³ @Temperature 563 - 563 °F |
Average value: 1.27 g/cc Grade Count:2 |
|
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
|
|||
| Density |
1.25
-
1.28
g/cc @Temperature 250 - 270 °C |
0.0452
-
0.0462
lb/in³ @Temperature 482 - 518 °F |
Average value: 1.26 g/cc Grade Count:2 |
|
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
|
|||
| Density | 1.10 - 1.28 g/cc | 0.0397 - 0.0462 lb/in³ | Average value: 1.19 g/cc Grade Count:7 |
|
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
|
|||
| Density | 1.22 - 1.28 g/cc | 0.0442 - 0.0463 lb/in³ | |
|
Lord Adhesives 4 No-Mix Accelerator for 200/500 Series
Lord Adhesives 4 No-Mix Accelerator for 200/500 SeriesLord Accelerator 4 is a no mix accelerator for Lord 200 and 500 series acrylic adhesives. Brush, wipe, spray or dip on one or both surfaces to b..
|
|||
| Density | 1.25 - 1.28 g/cc | 0.0452 - 0.0462 lb/in³ | |
|
Sibur 140-13P Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 85 Flexible PVC, Insulation
Low temperatures
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 56 Flexible PVC, Injection Molding for Footwear
Vamp boots
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 6814 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 7410 Flexible PVC, Injection Molding for Footwear
Sandals
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 7802 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 8502 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GSK 0637/AL Flexible PVC, Injection Molding, Lead Free
Items according to norm 2002/72/CE
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PMP 81 Flexible PVC, Extrusion Modified with PU
Under sheathing PVC/PU
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PMP 202 Flexible PVC, Extrusion Modified with PU
Undersheath PVC/PU (UL 90°)
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PMS 75 Flexible PVC, Lead Free
Gas pipes stabilized Ca-Zn
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 8202 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 5525 Flexible PVC, Lead Free
Profiles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 7010 Flexible PVC, Extrusion
Pipes and profiles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds MGS 91 Medical Flexible PVC, Injection Molding
Connectors and special components
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PG 6620 Flexible PVC, Extrusion Modified with Rubber
Profiles modified with rubber
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PK 7015/UV Flexible PVC, Lead Free
Outdoor profiles anti-UV
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 65/FR Flexible PVC, Lead Free
Spiral pipes, UL 94 Class V0
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 6805 Flexible PVC, Lead Free
Various profiles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 8010/S Flexible PVC, Lead Free
Shiny profiles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PM 82/FR Flexible PVC, Extrusion
Pipes, UL 94 Class V0
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GS 8004 Flexible PVC, Injection Molding for Footwear
Soles
|
|||
| Density | 1.24 - 1.28 g/cc | 0.0448 - 0.0462 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PH 92/UV Flexible PVC, Transparent Extrusion