| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
Nilit FRIANYL B63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific)
Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc..
|
|||
| Density | 1.30 - 1.90 g/cc | 0.0470 - 0.0686 lb/in³ | Average value: 1.44 g/cc Grade Count:196 |
|
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, ..
|
|||
| Density | 1.30 - 1.69 g/cc | 0.0470 - 0.0611 lb/in³ | Average value: 1.37 g/cc Grade Count:18 |
|
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific)
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 GF25 L BK 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
Shuman 930-05V0 White Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 (Asia Pacific)
LNP* Thermocomp* RF0079SZ is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific)
LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D 792 |
|
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific)
PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific)
PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP NF004 PC+ABS
LNP* THERMOCOMP* NF004 is a compound based on PC+ABS resin containing 20% Glass Fiber.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
Polyram PlusTek RA325G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced, Flame Retardant, Halogen Free
30% Glass-fiber reinforced, flame retardant halogen free Nylon 66 for injection molding applications.Information provided by Polyram.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
Wanhua Chemical Wanthane® WHT-7195 Polycaprolactone Based TPU
Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced
Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | |
|
Wolf Kunststoff ZEDEX® ZX-100A Polymer Alloy
Main Characteristics: Tough; Resilient; Soft; Low cost solutionApplications: Handling, Vessel and pump, Steel and Water, Chemical Engineering, Automitve Technology, Machine ToolsInformation provided..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)<
Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
DSM Arnite® T06 200 (extrusion) PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
Chem Polymer Chemlon 215 GVH Nylon 6, 15% Glass Fiber Reinforced
A glass fiber reinforced, flame retardant nylon 6. The material has a V0 flammability rating according to UL 94 testing procedure at thicknesses down to 1/16" (1.57mm).Data provided by the manufact..
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific)
LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ASTM-D792 |
|
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
|
|||
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Cycoloy® CE1810 PC+ABS
PC/ABS with high stiffness and low CTE.This data was supplied by SABIC-IP for the Americas region.
|
|||