| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
|
Plastcom SLOVAMID 6 GF 30 HI PA6, 30% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre and with the content of thermoplastic kaoutchouc. Application: impacted mouldings and mouldings with high strength a..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
|
Plastcom SLOVAMID 66/6 GF 20 PA66/6, 20% glass fibre
FeaturesChemically reinforced alloy PA 66 and PA 6 with 20 % glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and ..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
Polykemi AB SCANMID 6 B12^ F25 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Density | 1.32 - 1.63 g/cc | 0.0477 - 0.0589 lb/in³ | Average value: 1.42 g/cc Grade Count:51 |
|
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 118 |
|
Gharda Chemicals GATONE™ 5300 PEEK, High Viscosity Grade
(discontinued **)
High viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical propert..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM Data |
|
Dow Questra® WA206 High Heat Syndiotactic Polystyrene, 40% Glass Filled
(discontinued **)
QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792, ISO 1183 |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612
(Unverified Data**)
Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
|
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
|
Momentive Performance Materials RTV21 Pink General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009 PC
LNP* STAT-KON* DD0009 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP STAT-KON DE006 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE006 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East)
Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP STAT-KON PFD04 PA 6
LNP* STAT-KON* PFD04 is a compound based on Nylon 6 containing 20% Glass Fiber. Added feature of this grade is: Ellectrically Conductive.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
Stir SpA TP 78 GE OIL (PVC)
Application: Extrusion petrol-tight tubesInformation provided by STIR SpA
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY
Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
|
Techmer ES Plastiblend® ABS/PBT GF20
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | |
|
Eastman Eastapak 9921 PET
ISO data as provided by the manufacturer, Eastman Chemical
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
|
Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural
Information provided by Eurotec®
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Density | 1.32 - 1.36 g/cc | 0.0477 - 0.0491 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FRT 95 Flexible PVC, Insulation
Telephone and interphone cables
|
|||
| Density | 1.32 - 1.36 g/cc | 0.0477 - 0.0491 lb/in³ | ISO R 1183 |
|
Fainplast Compounds PK 8025 Flexible PVC, Lead Free
Sheat according to norm Fiat type 55251
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
|
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
|
|||
| Density | 1.32 - 1.46 g/cc | 0.0477 - 0.0527 lb/in³ | Average value: 1.38 g/cc Grade Count:7 |
|
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
|
|||