| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | |
|
Plastcom SLOVAMID 6 GF 25 FRC 3 PA6, 25% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 25 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
Nilit FRIANYL A63 CV40 Nylon 6.6 for injection molding, 40% carbon fiber reinforced
Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
Nilit FRIANYL A63 KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Density | 1.35 - 1.75 g/cc | 0.0488 - 0.0632 lb/in³ | Average value: 1.60 g/cc Grade Count:76 |
|
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
Pasargad Polymer Peyvand Pasamid 3P-H7130B Nylon 6/66, 30% Glass Fiber Reinforced
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin
Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® C 52G1 V25 Grey R7035 (XC 1329/A) PA6, DRY
Description: Polyamide 6, Glass-filled, glow-wire modified, color stabilized, lubricated for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Application..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP STAT-KON EE004 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* EE004 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | DIN 53479 |
|
Polyram PlusTek PD300G6 Nylon 12, 30% Glass Fiber
30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
|
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
|
Elektro-Isola Etronit IS Phenolic, Paper Reinforcement, Dark Brown, Sheets
Description: Very good high-voltage insulation material. Very high breakdown voltage, in particular parallel to the layers. Dimensionally stable.Application: Insulation material in high-voltage tap ..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6000 GS 30 HWUVCP 30% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30
Information provided by EMS Grivory
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Crastin® LW9320LM BK591 PBT+SAN
(Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320LM is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. It ha..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | JIS-Z-8807 |
|
Denka REOMER G G5082 Thermoplastic Elastomer, For Extrusion
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6600 CF30 HWCP 30% Carbon Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Side 1, Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 51576B015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 55989R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | |
|
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 51146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red sili..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Layer 2, Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Side 2, Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, ..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | Layer 1, Silicone Property; Arlon SQA-TMS-024 |
|
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792 |
|
Ashley Polymers Ashlene® 1420B Polycarbonate, 20% Glass Reinforced
A 20% glass reinforced polycarbonate for increased mechanical strength and thermal properties, modified for good impact with increased dimensional stability and overall toughness. 1423B with UV sta..
|
|||
| Density | 1.35 g/cc | 0.0488 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications
|
|||