| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics EXTEM UH1006M TPI Blend
High heat amorphous TPI Blend, Chemical Resistant
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**)
Zytel® FE270050 BK099 is a 30% glass reinforced, polyamide 66 resin for gas and water assisted injection molding.Information provided by DuPont
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | DIN 53479; ASTM D792 |
|
Kolon KOPA® KN333G33CR G/F Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This ..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK
LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP LX82803 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LX82803 is a compound based on Polyetheretherketone resin containing Proprietary Lubricant. Added features include : Internally Lubricated.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50
Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Techmer ES Electrafil® J-50/CF/20/TF/15 Polycarbonate, 20% Carbon Fiber Reinforced, 15% PTFE |
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6 GF33 L NAT004 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: Natural ColorTPCI# 9411102Informatio..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Stir SpA AF 95 HT 105 CZ (PVC)
Application: Extrusion insulation CEI 20-11 type TI3 and YI8Information provided by STIR SpA
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone
Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP DB0049R PC (Europe-Africa-Middle East)
LNP* Thermocomp* DB0049R is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12
LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 216 V30 Natural FA PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber and modified for enhanced injection molding.Available in: Europe Product Applications: This material offers an excellent combination b..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
|
Plenco 7500 Phenolic, Granular, Injection Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Polyram PlusTek RA331G6 Nylon 66 for Injection Molding, 30% Glass-Fiber Reinforced
30% Glass-fiber reinforced Nylon 66 for injection molding applications.Information provided by Polyram.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® TSM-30/2 PA666-MD30
Product description: Grilon TSM-30/2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral filler. Grilon TSM-30/2 has the following important properties: Excell..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)
(Unverified Data**)
Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | JIS-Z-8807 |
|
Denka VINYKON M4000 PVC, M grade for hard injection molding
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**)
30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded
BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Eurostar Staramide RF006S-GY9A121 PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006S-GY9A121 is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
|
|||
| Density | 1.37 g/cc | 0.0495 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOTUF WF003I Polyester, TP
LNP THERMOTUF* WF003I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.
|
|||