Polymer Property : Density = 1.39 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO data
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
Density 1.39 - 1.65 g/cc
0.0502 - 0.0596 lb/in³
Average value: 1.52 g/cc Grade Count:15
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Density 1.39 - 1.61 g/cc
0.0502 - 0.0582 lb/in³
Average value: 1.50 g/cc Grade Count:17
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Density 1.39 - 1.62 g/cc
0.0502 - 0.0585 lb/in³
Average value: 1.51 g/cc Grade Count:45
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC
LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare.
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)
Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific)
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength
Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Chengdu Polyster FH2040 Thermoplastic Polyether-ester Elastomer (TPEE)
Blend of H2040 and self-made flame retardant material. Excellent flex resistance at low temperatures. Excellent flex-fatigue resistance. Applications requiring flexibility at low temperatures and fl..
Density 1.39 g/cc
0.0502 lb/in³
ASTM D1505
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, ..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® E Polyester Film, 48 Gauge
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applicat..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® EC Polyester Film, 200 Gauge
Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® EL Polyester Film, 142 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® M461 Polyester Film, 200 Gauge
Mylar® M461 is a tough, general purpose, untreated polyester film. It is transparent in 48 through 300 gauge and translucent in heavier gauges. Mylar® M461 is based on DuPont Teijin Film's RSX fil..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® MDA Polyester Film, 1200 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® P25T Polyester Film, 75 Gauge
Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RSX951 Polyester Film, 105 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RSX951 Polyester Film, 48 Gauge
Mylar® RSX951 is a silicone coated polyester film designed for use as a release liner in various casting applications. The silicone release coating is applied to the film during the film production..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 284 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds CKL 173 Flexible PVC, Sheathing Lead Free
General purpose - good flexibility
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® EB11 Polyester Film, 48 Gauge
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is..
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® HR951 Polyester Film, 92 Gauge
Mylar® HR951 is a one-side release coated polyester film with good handling properties and clarity. It has been developed for use in various industrial applications.Information provided by DuPont.
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® RSX Polyester Film, 200 Gauge
Mylar® RSX films are slightly hazy, tough, general-purpose films. They have a rough surface to provide ease of handling, good adhesion, and processability. They are used for a broad range of indust..
Density 1.39 g/cc
0.0502 lb/in³
dry; ISO 1183
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
CENTROPLAST CENTROLYTE FG Polyethylene terephthalate, Food Grade
This material is electrically insulating, with good chemical resistance, high mechanical strength and wear resistance.Information provided by CENTROPLAST Engineering Plastics GMBH
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
DuPont Teijin Films Mylar® MDA Polyester Film, 200 Gauge
Mylar® MDA films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion..
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®