| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183/A |
|
Grupo Repol Dinalon® B1S25 G35 35% Glass Fiber Reinforced Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics ULTEM 2200F PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber
Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East)
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 GF/M40 B1 BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearan..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WC006 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS
LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP VERTON RX10409D PA 66
LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183-A |
|
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)
Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**)
UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions ..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | DAM; ISO 1183 |
|
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**)
43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D1505-85 |
|
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and va..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 100PE NC010A Acetal Homopolymer
Delrin® 100PE NC010A is a high viscosity acetal homopolymer, an enhanced version of Delrin® 100P with extremely low VOC emissions. It has improved processing thermal stability, good mechanical pro..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet
Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | |
|
DuPont™ Kapton® 200VN Polyimide Film, 50 Micron Thickness
Film thickness 50 micron 2.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available in..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET
Ultradur B 4040 G3 HT BK5830 is a 15% glass filled, pigmented black, injection molding PBT. It is a resin for molding household appliances and equipment which must be resistant to chemicals and oth..
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ASTM D792 |
|
Techmer ES HiFill FR® PBT FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
|
DuPont Performance Polymers Delrin® SC631 NC010 Acetal Homopolymer
(Unverified Data**)
Delrin® SC631 is a medium-high viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
|
|||