Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.43 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.20 - 1.43 g/cc
0.0434 - 0.0517 lb/in³
Average value: 1.28 g/cc Grade Count:10
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Density 1.06 - 1.43 g/cc
0.0383 - 0.0517 lb/in³
Average value: 1.10 g/cc Grade Count:49
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Density 1.11 - 1.43 g/cc
0.0401 - 0.0517 lb/in³
Average value: 1.21 g/cc Grade Count:7
Overview of materials for Polyphenylene Ether, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values ..
Density 1.43 - 1.43 g/cc
<br>@Temperature 215 - 215 °C
0.0517 - 0.0517 lb/in³
<br>@Temperature 419 - 419 °F
Average value: 1.43 g/cc Grade Count:1
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Density 1.21 - 1.43 g/cc
0.0437 - 0.0517 lb/in³
Average value: 1.30 g/cc Grade Count:10
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Density 1.36 - 1.43 g/cc
0.0491 - 0.0517 lb/in³
Average value: 1.40 g/cc Grade Count:31
Overview of materials for Phenolic, Novolac, Woodflour Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
SGL Carbon Group PANOX® FA C063 EEA High performance Crimped staple oxidized textile fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
SGL Carbon Group PANOX® FA C063 SSC High performance Crimped staple oxidized textile fiber, For felts and non-wovens
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
SGL Carbon Group PANOX® SA C063 EEA High performance oxidized textile fiber, Crimped staple fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
SGL Carbon Group PANOX® SA C063 SSC High performance oxidized textile fiber, Crimped staple fiber, For felts and non-wovens
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
Fiber Density
SGL Carbon Group PANOX® SA T320 EEA High performance oxidized textile fiber, Continuous Tow with 320k filaments
For carbon/carbon and spinning. PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not b..
Density 1.41 - 1.43 g/cc
0.0509 - 0.0517 lb/in³
Zell-Metall Engineering Plastics Zellamid 900 (POM-C)
Zellamid® 900 is the registered trademark of Zell-Metall’s high molecular weight Acetal resin.Acetal (POM) is noted for it’s high mechanical strength, heat resistance and good antifriction ..
Density 1.41 - 1.43 g/cc
0.0509 - 0.0517 lb/in³
Dry Density
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH
Zellamid® 900 is the registered trademark of Zell-Metall’s high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope..
Density 1.23 - 1.43 g/cc
0.0444 - 0.0517 lb/in³
Trelleborg Emerson & Cuming Eccobond® 45LV Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45LV Eccobond® Two-Component General Purpose Epoxy AdhesiveLow viscosity, filled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted ..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds CKL 012 Flexible PVC, Sheathing Lead Free
General purposes
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds CL 83/1 Flexible PVC, Sheathing
Sheath coaxial TV Cable
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds GK 90/R Flexible PVC, Flame Retardant Sheathing Lead Free
Hydrocarbon resistant
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds FR 95/1 Flexible PVC, Insulation
General purposes
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1184
Fainplast Compounds KL 0993 Flexible PVC, Insulation for High Temperatures Lead Free
Insulation
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds PK 96 Flexible PVC, Lead Free
Semi-rigid extrusion
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds PM 5580 Flexible PVC, Lead Free
Gaskets for frames
Density 1.38 - 1.43 g/cc
0.0499 - 0.0517 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 166 Phenolic Molding Chopped cotton fabric Filler, Compression Molded
Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BlackMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins..
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ASTM D792
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds AP 93 Flexible PVC, Flame Retardant Insulation
General purposes
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds CKL 182 Flexible PVC, Sheathing Lead Free
Sheathing coaxial cable (90°)
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds CKL 79 Flexible PVC, Sheathing Lead Free
General purposes
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds GA 86/R Flexible PVC, Flame Retardant Sheathing
Hydrocarbon resistant
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1183
Fainplast Compounds PM 65/R Flexible PVC, Lead Free
Extrusion modified with rubber
Density 1.39 - 1.43 g/cc
0.0502 - 0.0517 lb/in³
ISO R 1184
Fainplast Compounds RI 52/C Rigid PVC, Injection Molding
Electric fittings
Copyright © lookpolymers.com All Rights Reserved