| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
DSM Arnite® CCT GF20 (T-X01415) PBT-20% Glass Reinforced (European Grade)
(discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit..
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1184 |
|
Fainplast Compounds RKS 325 Rigid PVC, Antishock Extrusion Lead Free
Various profiles, antishock
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
Lanxess Pocan® KL 1-7033 000000 PBT, 30% Glass Fiber
PBT, 30% glass fibers, injection molding, impact modified
|
|||
| Density | 1.46 g/cc | 0.0528 lb/in³ | Laminate Density |
|
Hardwire 3SX-4-12 Low Density Composite
The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as w..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
Techmer ES HiFill® PA6/6 0146 A Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6
LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66
LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
SABIC Innovative Plastics LNP Thermocomp RF008U PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF008U is a compound based on PA 66 resin containing Glass Fiber. Added features include; UV-Stabilized, Easy Molding.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
|
Solvay TECHNYL® A 20 V35 PA66, 35% glass fiber, Conditioned
Description: Flame retardant polyamide 66, reinforced with 35% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America.Product Applications: This ph..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | DIN 53479 |
|
Polyram RamTal PM7013G2 Acetal, 10% Glass Fiber
10% Glass fiber reinforced and UV stabilized polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
EMS-Grivory Grivory® BG-40 S PA6-GF40
Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 92 Flexible PVC, Insulation
General purposes
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
Ascend Performance Materials VYDYNE® R220 Nylon, Mineral Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
|
Adell BR-18 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Density | 1.46 - 1.70 g/cc | 0.0527 - 0.0614 lb/in³ | Average value: 1.60 g/cc Grade Count:22 |
|
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | |
|
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b..
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
|
Fainplast Compounds HAX HF 28 Halogen Free PVC
Sheathing; good mechanical properties
|
|||
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
|
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
|
|||