Polymer Property : Density = 1.49 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 8699 BLK
Multi-Flex® A 8699 is a TPE compound based on Kraton G polymer. It is used as medium density acoustic for noise abatement in the auto industry. Multi-Flex TPE contains Kraton™ G.Data provided by..
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792, ISO 1183
Nilit Nilitop BT G2 FR C3 is a 10% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G2 FR C3 is a 10% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylon® N1040MGHL Nylon 6/6 (DAM)
Information provided by Ravago.
Density 1.49 g/cc
0.0538 lb/in³
DAM; ASTM D792
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (Cond)
Information provided by Ravago.
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylon® N2043L Nylon 6 (DAM)
Information provided by Ravago.
Density 1.49 g/cc
0.0538 lb/in³
Momentive Performance Materials RTV566 Red Extreme High Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-A
Solvay Technyl® A218V43 43% Glass Filled, Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183/A
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6
Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G..
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific)
LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive..
Density 1.49 g/cc
0.0538 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66
LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f..
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resist..
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly
LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal
LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass.
Density 1.49 g/cc
0.0538 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly
LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data ..
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Sax Polymers SAXAMID 126F9 Nylon 6, 45% Glass Fiber
SAXAMID 126F9 is a polyamide 6 injection-molding-grade reinforced with 45% glass fibers.Information provided by SAX Polymers
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Wellman EcoLon® 2200-BK1 Nylon 66, 40% Mineral/Glass Reinforced
All information provided by Wellman Engineered Resins.
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Wellman Wellamid® MRGF1882-BK1 Nylon 66, 40% Mineral/Glass Reinforced
All information provided by Wellman Engineered Resins.
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183-87
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Improved surface appearance gradeAll information provided by Wellman Engineered Resins.
Density 1.49 g/cc
0.0538 lb/in³
Nominal Laminate
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K
Fiber: HS Carbon, Plain Weave, 193 g/m2Information provided by HexCel
Density 1.49 g/cc
0.0538 lb/in³
(DAM); ISO 1183
DSM Akulon® K224-HGM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
DSM Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.49 g/cc
0.0538 lb/in³
dry; ISO 1183
DSM Novamid® 1013G45 1 NA PA6-GF45
45% Glass Reinforced, Injection Molding
Density 1.49 g/cc
0.0538 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..
Density 1.49 - 1.53 g/cc
0.0538 - 0.0553 lb/in³
ISO R 1183
Fainplast Compounds CL 82 Flexible PVC, Sheathing
General purposes
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Density 1.49 g/cc
0.0538 lb/in³
dry; ISO 1183
BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..
Density 1.49 g/cc
0.0538 lb/in³
dry; ISO 1183
BASF Ultramid® 8260 HS PA6 (Conditioned)
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Density 1.49 g/cc
0.0538 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Density 1.49 g/cc
0.0538 lb/in³
LATI Latilub 95-25GR CE/10 PSU, Mineral Fiber Reinforced, Graphite Filled