| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 - 1.50 g/cc | 0.0423 - 0.0542 lb/in³ | Average value: 1.28 g/cc Grade Count:46 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
|
|||
| Density | 1.14 - 1.50 g/cc | 0.0412 - 0.0542 lb/in³ | Average value: 1.24 g/cc Grade Count:33 |
|
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
|
|||
| Density | 1.13 - 1.50 g/cc | 0.0408 - 0.0542 lb/in³ | Average value: 1.30 g/cc Grade Count:12 |
|
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
|
|||
| Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | ISO 1183 |
|
Manifattura Cattaneo PVC U Polyvinyl Chloride
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Density | 1.00 - 1.50 g/cc | 0.0361 - 0.0542 lb/in³ | ASTM B212 |
|
H.C. Starck Amperit® 821.084 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
| Density | 1.30 - 1.50 g/cc | 0.0470 - 0.0542 lb/in³ | DIN 53479/A |
|
Stanelco Bioplast® Wrap 100 Biodegradable Plastic
Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated..
|
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
|
Sinotek Materials B Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
|
Sinotek Materials B Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
|
Sinotek Materials D Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 1.20 - 1.50 g/cc | 0.0434 - 0.0542 lb/in³ | ASTM D792 |
|
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy
EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl..
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CL 73 Flexible PVC, Sheathing
General purposes
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CL 76 Flexible PVC, Sheathing
Medium flexibility
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CL 86/1 Flexible PVC, Sheathing
Sheath coaxial TV Cable
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FK 0879 Flexible PVC, Insulation Lead Free
General purposes
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FK 90 Flexible PVC, Insulation Lead Free
General purposes
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 75 Flexible PVC, Insulation
General purposes
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds FR 92/1 Flexible PVC, Insulation
Power cables
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds GA 0248/4 Flexible PVC, Flame Retardant Sheathing
Hydrocarbon resistant sheathing
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1187 |
|
Fainplast Compounds GK 75 Flexible PVC, Flame Retardant Sheathing Lead Free
General purposes
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
|
Fainplast Compounds HAX HF 019/27 Halogen Free PVC
Sheathing; high flexibility
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
|
Fainplast Compounds HAX HF 039/31 Halogen Free PVC
Sheathing, insulation; high flexibility
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
|
Fainplast Compounds CKL 76 Flexible PVC, Sheathing Lead Free
General purposes
|
|||
| Density | 1.45 - 1.50 g/cc | 0.0524 - 0.0542 lb/in³ | |
|
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Density | 1.45 - 1.50 g/cc | 0.0524 - 0.0542 lb/in³ | |
|
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Density | 1.00 - 1.50 g/cc | 0.0361 - 0.0542 lb/in³ | ASTM B212 |
|
H.C. Starck Amperit® 821.6 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
|
Sinotek Materials A Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
|
Sinotek Materials C Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
|
Sinotek Materials D Graphite Roll
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
|
|||
| Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
|
Fainplast Compounds HAX HF 28 Halogen Free PVC
Sheathing; good mechanical properties
|
|||
| Density | 0.210 - 1.50 g/cc | 0.00759 - 0.0542 lb/in³ | Average value: 1.17 g/cc Grade Count:125 |
|
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..
|
|||