Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.51 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information..
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Plenco 4759 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 04759 is a black, two stage, medium heat resistant phenolic molding compound. It has excellent molded finish and possesses good electrical properties. It is used in appli..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183/A
Grupo Repol Dinalon® A1S25 G45 H PA66 45% Glass Fiber, Heat Stabilized
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP OCP36F PPS - Linear (Asia Pacific)
LNP LUBRICOMP* OCP36F is a compound based on PPS - Linear resin containing Bearing Grade, Carbon Fiber, Lubricants. Added features of this material include: Electrically Conductive.
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
Density 1.51 g/cc
0.0546 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp RFN18SXZ PA 66
LNP LUBRICOMP* RFN18SXZ is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Ameri..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Density 1.51 g/cc
0.0546 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT
LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region.
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber.
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES (Europe-Africa-Middle East)
LNP* Thermocomp* JF004E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP LF006EL PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006EL is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding. FDA Compliant Raw Materials.
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding.
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Plenco 4327 Phenolic, Granular, Compression Molded
PLENCO 04327 is a heat resistant mineral filled phenolic molding compound offering excellent cosmetic characteristics and improved heat resistant properties. PLENCO 04327 is not intended for electri..
Density 1.51 g/cc
0.0546 lb/in³
(DAM); ISO 1183
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Density 1.51 g/cc
0.0546 lb/in³
ASTM D1505
DuPont Teijin Films Melinex® 339 Polyester Film, 1000 Gauge
Melinex® 339 is an opaque white polyester film with good handling properties that is pre-treated on both surfaces to promote adhesion to most industrial coatings.Typical Applications: Melinex® 339..
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
IEC 60811
Fainplast Compounds HAX HF 029/47 Halogen Free PVC
General purpose
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
IEC 60811
Fainplast Compounds HAX HF 4021/TC Halogen Free PVC
Improved flame retardancy
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1184
Fainplast Compounds HGA 40 Flexible PVC, Sheathing for High Temperatures
Sheath high L.O.I.
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1184
Fainplast Compounds R 316/AS Rigid PVC, Extrusion
Antistatic profiles
Density 1.51 - 1.55 g/cc
0.0546 - 0.0560 lb/in³
ISO R 1183
Fainplast Compounds GA 90 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 30% glass fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance, e.g. automotive connect..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Conditioned, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Density 1.51 g/cc
0.0546 lb/in³
ISO 1183
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved