Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D955
Nylene® PA6 Glass Filled 5250 HS Nylon 6
50% Glass Filled; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Plenco 7527 Phenolic, Nodular, Injection Molded  (discontinued **)
Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer
LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL
LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183/A
Solvay TECHNYLSTARâ„¢ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: ..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP DF0079 PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF0079 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP KF004A Acetal Homopolymer
LNP THERMOCOMP* KF004A is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP QF0069 PA6.10 (Europe-Africa-Middle East)
LNP* THERMOCOMP* QF0069 is a compound based on PA610 resin contaning Glass Fiber, Flame Retardant. Added features include: Flame retardant.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East)
50% glass beads filled Polyamide 66 injection moulding resin.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Polyplastics Duranex® 7195W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Density 1.56 g/cc
0.0564 lb/in³
Toyobo Zylon® HM Poly(p-phenylene-2,6-benzobisoxazole) Fiber
Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using t..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Eurostar Starflam RF0059 PA66, Glass Fiber, Flame Retardant, Injection Molded
Starflam RF0059 is a Flame Retardant, Glass Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM
GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Density 1.56 g/cc
0.0564 lb/in³
Side 1; Arlon SQA-TMS-024
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat..
Density 1.56 g/cc
0.0564 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Density 1.56 g/cc
0.0564 lb/in³
Side 1 Cured Silicone Property; Arlon SQA-TMS-024
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh..
Density 1.56 g/cc
0.0564 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo..
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced
Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer
Density 1.56 g/cc
0.0564 lb/in³
Layer 2, Silicone Property; Arlon SQA-TMS-024
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Conditioned, 50% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
BASF Ultramid® A3WG10 BK 00564 50% Glass Filled PA66 (Conditioned)
Description: 50% glass-fiber reinforced injection-molding grade with high heat aging resistance for technical articles of very high stiffness.Information provided by BASF
Density 1.56 g/cc
0.0564 lb/in³
3M Scotchkote™ 445 Epoxy Slip Deterrent System
Scotchkote Epoxy Slip Deterrent System 445 has been specifically developed as a 100% solids system for use with 3M Scotchkote Granular Aggregate to provide a slip deterrent finish to high risk floor..
Density 1.56 g/cc
0.0564 lb/in³
(DAM); ISO 1183
DSM Akulon® K223-HMS6 Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Plenco 6527 Phenolic, Granular, Injection Molded
PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco.
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..