Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.60 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
PolyOne OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
PolyOne OnForce™ LFT NN-50LGF/000 HS UV Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Density 1.60 g/cc
0.0578 lb/in³
Average Density
Potters Industries Conduct-O-Fil® SH400S20 Silver-Coated Hollow Glass Spheres
Conduct-O-Fil® Conductive Particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. Applications include conductive paints and coatings, aerospac..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Density 1.60 g/cc
0.0578 lb/in³
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced  (discontinued **)
Key Features: Electrostatic DissipativeRosite Conductive C used in applications such as molded paper guides in printers and plotters. Conductive C is the UL recognition.Information provided by Onei..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Glastic Laminates/Shapes FHT Flexible High Temperature Polyester Laminate
Data provided by Glastic Corporation.Excellent flexibility plus good electrical strength retention values after long term heat aging. Widely used in motors and dry type transformers.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D572
Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet
A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registe..
Density 1.60 g/cc
<br>@Temperature 121 °C
0.0579 lb/in³
<br>@Temperature 250 °F
Dry Density
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 1.60 g/cc
0.0579 lb/in³
Wet Density
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable
Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or ..
Density 1.60 g/cc
0.0578 lb/in³
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 15% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific)
LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Techmer ES Electrablend® PA6 04001 FR MB Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated, Flame Retardant and Radio Frequen..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy
E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc.
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Plenco 4466 Phenolic, Granular, Compression Molded
PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466..
Density 1.60 g/cc
0.0578 lb/in³
Zircar Refractory Composites RS-A2 Refractory Sheet
This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee..
Density 1.60 g/cc
0.0578 lb/in³
Cured
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
E-Polymers TEKAMID® TB120G60W , 62% Glass Fiber Reinforced PA6, DAM
High strength, weather resistanceInformation provided by E-Polymers Co. Ltd.
Density 1.60 - 1.70 g/cc
0.0578 - 0.0614 lb/in³
ISO 1183
BASF Ultradur® B 4406 G3 Uncolored Q717 PBT
Information provided by BASF
Density 1.60 - 1.75 g/cc
0.0578 - 0.0632 lb/in³
Molding; IS 867-1963
Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color..
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DFL369XF PC (Asia Pacific)
LNP* Lubricomp* DFL369XF is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East)
LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding.
Density 1.60 g/cc
0.0578 lb/in³
Cured
Chesterton MRS 58 Metal Rebuilding System
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo..
Density 1.60 - 1.64 g/cc
0.0578 - 0.0592 lb/in³
ISO R 1184
Fainplast Compounds RE 235 Rigid PVC, Extrusion
Electric channels and profiles