Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.77 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg
The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and ..
Density 1.77 g/cc
0.0640 lb/in³
Parkway Products Thixomolded® AM50A Magnesium
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate..
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a..
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides..
Density 1.77 g/cc
0.0639 lb/in³
50% Resin Content; Internal Method
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy
The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Density 1.77 g/cc
0.0640 lb/in³
Yield Density
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 850 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D572
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced
The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compressio..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Kureha KF Polymer 2950 PVDF Copolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 0177 Nylon 66
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Techmer ES HiFill® PA6/6 GF60 TL10 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 8575101Information provi..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Sumitomo Bakelite Sumikon® PM-9640 Glass Filled Phenolic
Two stage glass fiber filled black phenolic. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. PM-9640 is widely used in ..
Density 1.77 g/cc
0.0639 lb/in³
ASTM D792
Westlake Plastics Kynar® PVDF CN-F Polyvinylidene Fluoride (conductive)
Non-sloughing carbon-fiber-filled material with resistance to most chemicals and solvents mechanically strong and tough, thermally stable to 335F, flame and abrasion resistant, and easily fabricated..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
DSM Stanyl® 46HF5040 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America)
Information provided by DSM Engineering Plastics.
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.77 g/cc
0.0639 lb/in³
ISO 1183
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65
Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami..
Density 1.77 g/cc
0.0639 lb/in³
Cytec Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Density 1.77 g/cc
0.0640 lb/in³
ASTM D792
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products
Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent..
Density 1.77 - 1.79 g/cc
0.0639 - 0.0647 lb/in³
ASTM D792
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Density 1.77 g/cc
0.0639 lb/in³
Arkema Group Kynar® 1000 HDC N 118 PVDF  (discontinued **)
Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig..
Density 1.77 g/cc
0.0639 lb/in³
Arkema Group Kynar® FLEX 2822 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EDN, N. ?E5.C.H.B.C,, ? (4-8)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousness ..