Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.82 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
Density 1.82 g/cc
0.0658 lb/in³
Cookson Group Plaskon® S-7P Epoxy Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically ..
Density 1.82 g/cc
0.0658 lb/in³
Cookson Group Plaskon® S-7S Epoxy Encapsulant  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically ..
Density 1.82 g/cc
0.0658 lb/in³
IDI Composites E-203 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
Density 1.82 g/cc
0.0658 lb/in³
Fiber Density
SGL Carbon Group SIGRAFIL C® C30 S006 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Density 1.82 g/cc
0.0658 lb/in³
Fiber Density
SGL Carbon Group SIGRAFIL C® C30 S009 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Density 1.82 g/cc
0.0658 lb/in³
Fiber Density
SGL Carbon Group SIGRAFIL C® C30 S012 GLY Staple Carbon Fiber, Glycerine Sizing
In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making..
Density 1.82 g/cc
0.0658 lb/in³
ASTM D891
Solvay Specialty Polymers FOMBLIN® Z03 PFPE Lubricant
FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc...
Density 1.82 g/cc
<br>@Temperature 25.0 °C
0.0658 lb/in³
<br>@Temperature 77.0 °F
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Density 1.82 g/cc
0.0658 lb/in³
Specialty Materials Hy-Bor 100 Boron/Graphite Hybrid Prepreg Tape
Lower cost Hy-Bor version. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 m..
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc.
Density 1.82 g/cc
0.0658 lb/in³
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.82 g/cc
0.0658 lb/in³
Relative Density; ISO 1183
Vyncolit G885 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group
Density 1.82 g/cc
0.0658 lb/in³
Cosmic Plastics D72 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.82 g/cc
0.0658 lb/in³
(DAM); ISO 1183
DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
Density 1.82 g/cc
0.0658 lb/in³
ISO 1183
DSM Stanyl® TE250F9 (DAM) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Information provided by DSM Engineering Plastics.
Density 1.82 g/cc
0.0658 lb/in³
(DAM); ISO 1183
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.82 g/cc
0.0658 lb/in³
Bond Laminates TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Density 1.82 g/cc
0.0658 lb/in³
Liquid
3M Fluorinert™ FC-3283 Electronic Liquid
3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor..
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Applied Composites 8061 Polyester SMC
Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped Fibers, High Stiffness, High Fiber LoadingsInformation provided by Applied Composites Corp..
Density 1.82 g/cc
0.0658 lb/in³
Bond Laminates TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
Within the TEPEX® composite laminate, TPU distinguishes itself from alternative resin systems by its specific physical properties. The TPU resin is tough which results in an excellent impact and ea..
Density 1.82 g/cc
<br>@Temperature 0.000 °C
0.0658 lb/in³
<br>@Temperature 32.0 °F
Liquid
3M Novec™ 774 Engineered Fluid
3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high..
Density 1.82 g/cc
0.0658 lb/in³
DIN 53 47
Albis Plastics Tedur® L 9560 PPS, 50% Mineral
High Gloss, Highest Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Various High Temperature ReflectorsProcessing: Inje..
Density 1.82 g/cc
0.0658 lb/in³
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..
Density 1.82 g/cc
0.0658 lb/in³
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.82 - 1.84 g/cc
0.0658 - 0.0665 lb/in³
ISO 1183
Polyplastic Armoflen® PO MF 75-1 Polypropylene Homopolymer, 75% Calcium Carbonate
Information provided by PolyPlastic Group.
Density 1.82 g/cc
0.0658 lb/in³
Dry As Molded
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH &
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high ..
Copyright © lookpolymers.com All Rights Reserved